Electrochemical polarization experiments were performed on Si wafers in ammoniacal solutions maintained at a pH in the range of 9.5 to 11.5. Anodic polarization of silicon yielded curves which are typical for materials that undergo passivation. The values of open circuit potential and passivation potential for p-type Si wafers were more anodic than for the n-type Si wafers. Corrosion current density of p-type Si wafers of low resistivity was lower than that of wafers of high resistivity. Corrosion current densities correlated well with surface roughness induced in alkaline solutions. Addition of surfactant or H2O2 to alkaline solutions reduced critical current density for passivation and corrosion current density.

Type
Research Article
Copyright
Copyright © Materials Research Society 1995

Access options

Get access to the full version of this content by using one of the access options below. (Log in options will check for institutional or personal access. Content may require purchase if you do not have access.)

References

REFERENCES

[1] Zhang, X. G., Collins, S. D., and Smith, R. L., J. Electrochem. Soc., 136, 1561 (1989).Google Scholar
[2] Smith, R. L., Kloeck, B., and Collins, S. D., J. Electrochem. Soc., 135, 2001 (1988).Google Scholar
[3] Allongue, P., Costa-Kieling, V., and Gerischer, H., J. Electrochem. Soc., 140, 1009 (1993).Google Scholar
[4] Siedel, H., Csepregi, L., Heuberger, A., and Baumgartel, H., J. Electrochem. Soc., 137, 3612 (1990).Google Scholar
[5] Sundaram, K. B. and Chang, H., J. Electrochem. Soc., 140, 1592 (1993).Google Scholar
[6] Chen, L., Chen, M., Lien, C., and Wan, C., J. Electrochem. Soc., 142, 170 (1995).Google Scholar
[7] Jeon, J. S., Raghavan, S., and Sperline, R. P., J. Electrochem. Soc., 142, 621 (1995).Google Scholar
[8] Palik, E. D., Glembocki, O. J., and Heard, I. Jr, J. Electrochem. Soc., 134, 404 (1987).Google Scholar