Evaluation of Ultra-thin Layer Fabricated by Wet-process as a Pore-Seal for Porous Low-k Films

Published online by Cambridge University Press:  29 July 2011

Shoko Sugiyama Ono
Affiliation:
R&D Center, Mitsui Chemicals, Inc., Japan
Kazuo Kohmura
Affiliation:
R&D Center, Mitsui Chemicals, Inc., Japan
Hirofumi Tanaka
Affiliation:
R&D Center, Mitsui Chemicals, Inc., Japan
Yasuhisa Kayaba
Affiliation:
Research Institute for Nanodevice and Bio Systems, Hiroshima University, Japan
Takamaro Kikkawa
Affiliation:
Research Institute for Nanodevice and Bio Systems, Hiroshima University, Japan
Get access

Abstract

We focused on detailed evaluations of properties of the ultra-thin pore-seal layer (< 3 nm-thick), such as Cu diffusion barrier property and thermal stability. Cu diffusion into dense thermal silica and porous silica low-k which are covered with the pore seal layer was evaluated using metal-insulator-semiconductor (MIS) capacitors under bias thermal stress (BTS). Triangular voltage sweep (TVS) measurement shows that the ultra-thin layer on dense thermal silica suppresses the drift of Cu ions. The Time-Dependent Dielectric Breakdown (TDDB) lifetime of porous silica low-k covered with the ultra-thin pore seal layer results in a drastic increase of the capacitor lifetime with respect to the no-pore-seal control system (stable at 125 °C at least for 10000 s). Thermal decomposition of bulk material of the pore sealant was measured by thermal gravity (TG) test in nitrogen. Bulk material did not decompose through around 350 °C. The amount of ultra-thin pore seal layer fabricated on silicon wafer after thermal cycle stress in vacuum was measured by x-ray photoelectron spectroscopy (XPS). Amount of pore sealant did not decrease even after 2 cycles of 20 min, at 250 °C. Those results show that the ultra-thin layer, which we propose here, has a potential as a pore seal layer for porous low-k films.

Type
Research Article
Copyright
Copyright © Materials Research Society 2011

Access options

Get access to the full version of this content by using one of the access options below. (Log in options will check for institutional or personal access. Content may require purchase if you do not have access.)

References

REFERENCES

1. Caro, A. M., Maes, G., Borghs, G., and Whelan, C., Microelectron. Eng. 85(10), 20472050 (2008).Google Scholar
2. Gandhi, D. D., Lane, M., Zhou, Y., Singh, A. P., Nayak, S., Tisch, U., Eizenberg, M., and Ramanath, G., Nature 447(7142), 299U292 (2007).Google Scholar
3. Ganesa, P. G., Singh, A. P., and Ramanath, G., Appl. Phys. Lett. 85(4), 579581 (2004).Google Scholar
4. Caro, A. M., Maes, G., Borghs, G., Armini, S., and Travaly, Y., Mater. Res. Soc. Symp. Proc. 1249-F02-01 (2010).Google Scholar
5. George, S. M., Yoon, B., and Dameron, A. A., Acc. Chem. Res. 42(4), 498508 (2009).Google Scholar
6. Loscutoff, P. W., Zhou, H., Clendenning, S. B., and Bent, S. F., ACS Nano 4(1), 331341 (2010).Google Scholar
7. Loscutoff, P. W., Clendenning, S. B., and Bent, S. F., Mater. Res. Soc. Symp. Proc. 1249-F02-03 (2010).Google Scholar
8. Hijioka, K., Inoue, N., Kume, I., Kawahara, J., Furutake, N., Shirai, H., Itoh, T., Ogura, T., Kazama, K., Yamamoto, Y., Kasama, Y., Katsuyama, H., Manabe, K., Yamamoto, H., Saito, S., Hase, T., and Hayashi, Y., IEDM10–756.Google Scholar
9. Ono, S. S., Kohmura, K., Tanaka, H., Nakayama, K., Kagayama, A., Tsuchiya, T., Nakaura, M., Matsuoka, O., Takaki, T. and Maekawa, K., Mater. Res. Soc. Symp. Proc. 1249-F06-03 (2010).Google Scholar
10. Cui, H., Burke, P. A., Appl. Phys. Lett. 84 (14), 2629 (2004).Google Scholar
11. Chen, L. S., Bang, W. H., Park, Y.-J., Ryan, E. T., King, S., and Kim, C.-U., Appl. Phys. Lett. 96, 091903 (2010).Google Scholar