Enhanced Spontaneous Polarization of Dysprosium-substituted Lead Zirconate Titanate Thin Films by a Chemical Solution Deposition Method

Published online by Cambridge University Press:  01 February 2011

Hiroshi Uchida
Affiliation:
Department of Chemistry, Faculty of Science and Technology, Sophia University, 7–1 Kioi-cho, Chiyoda-ku, Tokyo, 102–8554, Japan
Hiroshi Nakaki
Affiliation:
Department of Chemistry, Faculty of Science and Technology, Sophia University, 7–1 Kioi-cho, Chiyoda-ku, Tokyo, 102–8554, Japan
Shoji Okamoto
Affiliation:
Department of Innovative and Engineered Materials, Tokyo Institute of Technology, 4259 Nagatsuta, Midori-ku, Yokohama, 226–8502, Japan
Shintaro Yokoyama
Affiliation:
Department of Innovative and Engineered Materials, Tokyo Institute of Technology, 4259 Nagatsuta, Midori-ku, Yokohama, 226–8502, Japan
Hiroshi Funakubo
Affiliation:
Department of Innovative and Engineered Materials, Tokyo Institute of Technology, 4259 Nagatsuta, Midori-ku, Yokohama, 226–8502, Japan
Seiichiro Koda
Affiliation:
Department of Chemistry, Faculty of Science and Technology, Sophia University, 7–1 Kioi-cho, Chiyoda-ku, Tokyo, 102–8554, Japan
Get access

Abstract

Influences of the B-site substitution using Dy3+ ion on the crystal structure and ferroelectric properties of lead zirconate titanate (PZT) films were investigated. Dy3+-substituted PZT films with nominal chemical compositions of Pb1.00Dyx (Zr0.40Ti0.60)1-(3x/4)O3 (x = 0 ∼ 0.06) were fabricated by a chemical solution deposition (CSD). Polycrystalline PZT films with preferential orientation of (111)PZT were obtained on (111)Pt/TiO2/SiO2/(100)Si substrates, while epitaxially-grown (111)PZT films were fabricated on (111)SrRuO3//(111)Pt//(100)YSZ//(100)Si substrate. Ratio of PZT lattice parameters (c/a), which corresponds to its crystal anisotropy, was enhanced by the Dy3+-substitution with x = 0.02. Spontaneous polarization (Ps) of Dy3+-substituted PZT film (x = 0.02) along polar [001] axis of PZT lattice was estimated from saturation polarization (Psat) value of the epitaxially-grown (111)PZT film on (111)SrRuO3//(111)Pt//(100)YSZ//(100)Si to be 84 μC/cm2 that was significantly larger than that of non-substituted PZT (= 71 μC/cm2). We concluded that the enhancement of Ps value could be achieved by the Dy3+-substitution that promoted the crystal anisotropy of PZT lattice.

Type
Research Article
Copyright
Copyright © Materials Research Society 2005

Access options

Get access to the full version of this content by using one of the access options below. (Log in options will check for institutional or personal access. Content may require purchase if you do not have access.)

References

REFERENCES

1. Watanabe, H., Mihara, T., Yoshimori, H. and Paz de Araujo, C. A.: Jpn. J. Appl. Phys. 34 (1995) 5240.Google Scholar
2. Furuya, A. and Cuchiaro, J. D.: J. Appl. Phys. 84 (1998) 6788.Google Scholar
3. Park, B. H., Kang, B. S., Bu, S. D., Noh, T. W., Lee, J. and Jo, W.: Nature 401 (1999) 682.Google Scholar
4. Noguchi, Y. and Miyayama, M.: Appl. Phys. Lett. 78 (2001) 1903.Google Scholar
5. Kojima, T., Sakai, T., Watanabe, T., Funakubo, H., Saito, K. and Osada, M.: Appl. Phys. Lett. 80 (2002) 2764.Google Scholar
6. Uchida, H., Yoshikawa, H., Okada, I., Matsuda, H., Iijima, T., Watanabe, T. and Funakubo, H.: Jpn. J. Appl. Phys. 41 (2002) 6820.Google Scholar
7. Tominaga, K., Shirayanagi, A., Takagi, T. and Okada, M.: Jpn. J. Appl. Phys. 32 (1993) 4082.Google Scholar
8. Kamiya, T.: Dr. Thesis, Department of Inorganic Materials, Tokyo Institute of Technology, Tokyo, 1996.Google Scholar
9. Hacccart, I., Remiens, D. and Callan, E.: Thin Solid Films 423 (2003) 235.Google Scholar
10. Kurchania, R. and Milne, S. J.: J. Sol-gel Sci. Tech. 28 (2003) 143.Google Scholar
11. Zhang, Q. and Whatmore, R. W.: Mater. Sci. Eng. B109 (2004) 136.Google Scholar
12. Choi, W. Y., Ahn, J. H., Lee, W. J. and Kim, H. G.: Mater. Lett. 37 (1998) 119.Google Scholar
13. Wu, L., Lee, C. C., Wu, T. S., Wei, C. C.: Ferroelectrics 41, (1982) 157.Google Scholar
14. Park, H. B., Park, C. Y., Hong, Y. S., Kim, K. and Kim, S. J.: J. Am. Ceram. Soc. 82 (1999) 94.Google Scholar
15. Garg, A. and Agrawel, D. C.: Mater. Sci. Eng. B86 (2001) 134.Google Scholar
16. Nakaki, H., Uchida, H., Yokoyama, S., Funakubo, H. and Koda, S.: Jpn. J. Appl. Phys. 43 (2004) 6558.Google Scholar
17. Saito, K., Oikawa, T., Kurosawa, T., Akai, T. and Funakubo, H.: Jpn. J. Appl. Phys. 41 (2002) 6730.Google Scholar
18. Yang, F., Bao, P., Chang, H. L. W., Choy, C. L. and Wang, Y.: Thin Solid Films 406 (2002) 282.Google Scholar
19. Okamoto, S., Watanabe, T., Morioka, H., Yokoyama, S., Akiyama, K., Muranaka, K., Horita, S. and Funakubo, H.: Ext. Abstr. (64th Autumn Meet. 2003); Japan Society of Applied Physics and Related Societies, 2a-V8. (in Japanese)Google Scholar
20. Morioka, H., Yokoyama, S., Oikawa, T. and Funakubo, H.: Appl. Phys. Lett. 85 (1999) 3516.Google Scholar