Hostname: page-component-586b7cd67f-t7fkt Total loading time: 0 Render date: 2024-11-25T17:40:42.275Z Has data issue: false hasContentIssue false

Crystallinity and Wet Etch Behavior of HfO2 Films Grown by MOCVD

Published online by Cambridge University Press:  01 February 2011

Katherine L. Saenger
Affiliation:
IBM Semiconductor R & D Center, IBM T.J. Watson Research Center, Yorktown Heights, NY
Cyril Cabral Jr
Affiliation:
IBM Semiconductor R & D Center, IBM T.J. Watson Research Center, Yorktown Heights, NY
Paul C. Jamison
Affiliation:
IBM Semiconductor R & D Center, IBM T.J. Watson Research Center, Yorktown Heights, NY
Edward Preisler
Affiliation:
IBM Semiconductor R & D Center, IBM T.J. Watson Research Center, Yorktown Heights, NY
Andrew J. Kellock
Affiliation:
IBM Almaden Research Center, San Jose, CA.
Get access

Abstract

The crystallinity and wet etching behaviors of ultrathin (<10 nm) HfO2 films grown by metal organic chemical vapor deposition (MOCVD) were examined as a function of deposition temperature, film thickness, and post-deposition annealing. Films 3 nm in thickness deposited at 400 or 500 °C were amorphous as-deposited and slowly etchable in aqueous HF; after annealing at 700 °C, the same films showed some nanocrystallinity and were impervious to HF. However, thicker films grown under the same conditions showed significant crystallinity and were impervious to HF even as-deposited. These observations, in combination with measurements on various samples etched back by an Ar+ ion damage/wet etch process, suggest a film structure comprising an initially amorphous near-interface region capped with a HF-resistant crystalline upper layer. It was found that the initially amorphous near-interface region (the bottom 1–3 nm) of films grown at 500 °C can be induced to at least partially crystallize as the upper part of the film starts becoming crystalline as-deposited, but that this near-interface region remains at least partially amorphous after annealing at 700°C.

Type
Research Article
Copyright
Copyright © Materials Research Society 2004

Access options

Get access to the full version of this content by using one of the access options below. (Log in options will check for institutional or personal access. Content may require purchase if you do not have access.)

References

REFERENCES

1. Gousev, E.P., Cabral, C. Jr, Copel, M., D'Emic, C., and Gribelyuk, M., Microelectronic Engineering 69 145 (2003).Google Scholar
2. Ho, M.-Y., Gong, H., Wilk, G.D., Busch, B.W., Green, M.L., Voyles, P.M., Muller, D.A., Bude, M., Lin, W.H., See, A., Loomans, M.E., Lahiri, S.K., and Raisanen, P.I., J. Appl. Phys. 93 1477 (2003).Google Scholar
3. Hausmann, D.M. and Gordon, R.G., J. Crystal Growth 249 251 (2003).Google Scholar
4. Saenger, K.L., Okorn-Schmidt, H.F., and D'Emic, C.P., Mat. Res. Soc. Symp. Proc. 745 79 (2003).Google Scholar