Extract

See analyses of the following items in microfiche Table 9, where details of sample number and context are also given. See also full catalogue of metallurgical debris in Table 2.

52. 5 fragments of lining material (18 g).

53. 8 fragments; probably pieces of vitrified lining material with Cu stains (8 .00 g); possibly just over-fired crucible.

54. 15 fragments of fuel ash slag (8.3 g), some copper stained. Analysis indicates copper-working slag.