A transient response technique has been employed to investigate the lifetime of free polarons in bulk heterojunction blends of regioregular poly (3-hexylthiophene) (P3HT) and [6,6]-phenyl-C61 butyric acid methylester (PCBM) at different annealing temperatures. Device efficiency and charge mobility were also measured. The longest lifetime, ∼ 1.5 microseceonds, was achieved for an annealing temperature of 140˚C; this represents a 2.5 x increase in lifetime relative to unannealed samples. The 140˚C annealing temperature also yields the highest efficiency. These measurements provide an estimate of the mobility-lifetime product, a figure of merit for charge transport in organic bulk heterojunctions.
Keywords
- Type
- Research Article
- Information
- MRS Online Proceedings Library (OPL) , Volume 1322: Symposium B – Third-Generation and Emerging Solar-Cell Technologies , 2011 , mrss11-1322-b09-11
- Copyright
- Copyright © Materials Research Society 2011
References
REFERENCES
- 2
- Cited by