Hostname: page-component-586b7cd67f-t7fkt Total loading time: 0 Render date: 2024-11-25T17:33:32.075Z Has data issue: false hasContentIssue false

Surface Electrochemistry of Uranium Dioxide in Acidic Hydrogen Peroxide Solutions

Published online by Cambridge University Press:  27 March 2012

Mayuri Razdan
Affiliation:
Department of Chemistry, University of Western Ontario, London, ON N6A 5B7, Canada
David Hall
Affiliation:
Department of Chemistry, University of Ottawa, Ottawa, ON K1N 6N5, Canada
David W. Shoesmith
Affiliation:
Department of Chemistry, University of Western Ontario, London, ON N6A 5B7, Canada
Get access

Abstract

The electrochemical reduction of H2O2 on SIMFUEL was investigated over the pH range 1 to 4. The mechanism at pH 4 is known to occur on UV species incorporated into a surface layer of UIV1-2xUV2xO2+x. However, below pH 3, reduction occurs on an adsorbed UVO2(OH) state which is unstable and oxidizes to insulating UVI before dissolving as UO22+. Both schemes are observed at intermediate pH’s. The presence of both low and high acidic regions at the electrode surface is determined by the combination of peroxide concentration, bulk pH and the surface diffusion conditions.

Type
Articles
Copyright
Copyright © Materials Research Society 2012

Access options

Get access to the full version of this content by using one of the access options below. (Log in options will check for institutional or personal access. Content may require purchase if you do not have access.)

References

REFERENCES

1 Nuclear Waste Management Organization (NWMO), Choosing a way forward: the future management of Canada’s used nuclear fuel. November, 2005. (www.nwmo.ca).Google Scholar
2 McMurry, J., Dixon, D.A., Garroni, J.D., Ikeda, B.M., Stroes-Gascoyne, S., Baumgartner, P., and Melnyk, T.W., Evolution of a Canadian deep geologic repository: Base scenario. Ontario Power Generation report: 06819-REP-01200-10092-R00 (2003).Google Scholar
3 King, F. and Kolar, M., The copper container corrosion model used in AECL’s second case study. Ontario Power Generation report: 06819-REP-01200-10041-R00, (2000).Google Scholar
4 Shoesmith, D. W., Kolar, M. and King, F., Corrosion 59, 802 (2003).10.5006/1.3277609Google Scholar
5 Amme, M., Radiochim. Acta 90, 399 (2002).10.1524/ract.2002.90.7_2002.399Google Scholar
6 Amme, M., Renker, B., Schmid, B., Feth, M. P., Bertagnolli, H., and Dobelin, W., J. Nucl. Mater. 306, 202 (2002).10.1016/S0022-3115(02)01291-6Google Scholar
7 Diaz-Arocas, P., Quinones, J., Maffiotte, C., Serrano, J., Garcia, J., Almazan, J. R., and Esteban, J., Mater Res. Soc. Symp. Proc. 353, 641 (1995).10.1557/PROC-353-641Google Scholar
8 Hiskey, J. B., Inst. Min. Metall. Trans. Sect. C, 89, C145 (1980).Google Scholar
9 Wren, J. C., Shoesmith, D. W. and Sunder, S., J. Electrochem. Soc. 152, B470 (2005).10.1149/1.2047349Google Scholar
10 Shoesmith, D. W., Noël, J. J., Garisto, F., Mater. Res. Soc. Symp. Proc. 824, 81 (2004).10.1557/PROC-824-CC2.3Google Scholar
11 Keech, P. G., Noel, J. J., and Shoesmith, D. W., Electrochim. Acta 53, 5675 (2008).10.1016/j.electacta.2008.03.008Google Scholar
12 Grenthe, I., Fuger, J., Konings, R. J., Lemire, R. J., Muller, A. B., Nguyen-Trung, C., and Wanner, H., in Chemical Thermodynamics Vol 1, edited by Wanner, H. and Forest, I., (North Holland, Amsterdam, 1992).Google Scholar
13 Lucuta, P. G., Verrall, R. A., Matzke, H., and Palmer, B. J., J. Nuc. Mater. 178, 48 (1991).10.1016/0022-3115(91)90455-GGoogle Scholar
14 Santos, B. G., Nesbitt, H. W., Noel, J. J., and Shoesmith, D. W., Electrochim. Acta 49, 1863 (2004).10.1016/j.electacta.2003.12.016Google Scholar
15 Shoesmith, D. W., J. Nucl. Mater. 282, 1 (2000).10.1016/S0022-3115(00)00392-5Google Scholar
16 Shoesmith, D. W., Sunder, S., and Hocking, W. H., in Electrochemistry of novel materials Vol 297, edited by Lipkowski, J. and Ross, P. N., (VCH, New York, 1994), chapter 6.Google Scholar
17 Goldik, J. S., Nesbitt, H. W., Noel, J. J., and Shoesmith, D. W., Electrochim. Acta 49, 1699 (2004).10.1016/j.electacta.2003.11.029Google Scholar
18 Goldik, J. S., Shoesmith, D. W., and Noel, J. J., J. Electroanal. Chem. 582, 241 (2005).10.1016/j.jelechem.2004.11.007Google Scholar
19 Lemire, R. J. and Paquette, J., Nuc. Sci. Eng. 79, 23 (1981).Google Scholar
20 Goldik, J. S., Noel, J. J., and Shoesmith, D. W., J. Electrochem. Soc. 153, E151 (2006).10.1149/1.2213419Google Scholar