Studies of Silane Adhesion Promoters on Silica Filler Particles for use in Microelectronic Packaging

Published online by Cambridge University Press:  17 March 2011

Maura Jenkins
Affiliation:
Department of Materials Science and Engineering, Stanford University, Stanford, CA 94305, U.S.A.
Gretchen DeVries
Affiliation:
Department of Materials Science and Engineering, Stanford University, Stanford, CA 94305, U.S.A.
Reinhold H. Dauskardt
Affiliation:
Department of Materials Science and Engineering, Stanford University, Stanford, CA 94305, U.S.A.
John C. Bravman
Affiliation:
Department of Materials Science and Engineering, Stanford University, Stanford, CA 94305, U.S.A.
Get access

Abstract

To avoid delamination which often occurs in microelectronic packaging as a result of widely varying thermal expansion coefficients, epoxy underfill is often loaded with particulate silica filler. This filler typically complicates the fracture behavior of the epoxy and surrounding layers. However, delamination of interfaces within the composite may contribute to toughening if the fracture path is adhesive between the epoxy and surrounding layers or otherwise removed from filler-epoxy delamination regions. In this work, the interface between silica filler and epoxy is altered with the use of silane coupling agents to elucidate the fracture and toughening mechanisms of filled epoxies. Two model epoxies are investigated, and coupling agents were chosen to encourage chemical reaction with each system. For the aliphatic epoxy system, coupling agents were identified which both augment and degrade the interface between filler and epoxy. In composite structures, it was observed that those coupling agents which degrade the filler-epoxy interface act as toughening agents. SEM indicates that most deformation is not at the filler-epoxy interface, but rather through the epoxy, very close to the filler particle surfaces. In contrast, no coupling agents were identified which act as toughening agents in the bisphenol-f system. Further, no variation in fracture toughness of composite structures was observed with the use of coupling agents, indicating that filler-epoxy delamination does not occur in this system. With few exceptions, SEM supports this interpretation.

Type
Research Article
Copyright
Copyright © Materials Research Society 2002

Access options

Get access to the full version of this content by using one of the access options below. (Log in options will check for institutional or personal access. Content may require purchase if you do not have access.)

References

REFERENCES

1. Kook, S.Y., Snodgrass, J.M., Kirtikar, A., Dauskardt, R.H., Journal of Electronic Packaging, Transactions of the ASME (1998).Google Scholar
2. Plueddemann, E.P. Silane Coupling Agents. 2nd ed. (Plenum, New York, 1991).Google Scholar
3. Kaas, R. L., and Kardos, J. L., Polymer Engineering and Science. 11, 11 (1971).Google Scholar