Article contents
SiC TO SiC WAFER BONDING
Published online by Cambridge University Press: 11 February 2011
Abstract
SiC wafers with an RMS roughness of 1.5 nm were bonded in a dedicated ultrahigh vacuum bonding chamber. Successful fusion of wafers was observed at temperatures as low as 800°C under a uniaxial mechanical stress of 20 MPa. Cross-section transmission electron microscopy (XTEM) of a specimen bonded at 1100°C revealed parts of the interface where wafers were in intimate contact, while other parts contained an up to 3 nm thick amorphous carbon interlayer. The bonded SiC retained its high crystalline quality; no extended defects emanating from the interface were observed within the sampling region. Electrical measurements showed that the azimuthal orientation of the bonded couple significantly influences the electrical character of the junction.