Selective Doping of 4H-SiC by Aluminum/Boron Co-diffusion

Published online by Cambridge University Press:  21 March 2011

Ying Gao
Affiliation:
University of South Carolina, Department of Electrical Engineering, Columbia, SC 29208, U.S.A.
S. I. Soloviev
Affiliation:
University of South Carolina, Department of Electrical Engineering, Columbia, SC 29208, U.S.A.
X. Wang
Affiliation:
University of South Carolina, Department of Electrical Engineering, Columbia, SC 29208, U.S.A.
C. C. Tin
Affiliation:
Auburn University, Physics Department, Auburn, AL 36849, U.S.A.
T. S. Sudarshan
Affiliation:
University of South Carolina, Department of Electrical Engineering, Columbia, SC 29208, U.S.A.
Get access

Abstract

Based upon graphite mask, selective aluminum/boron doping of SiC by thermal diffusion has been successfully realized in a temperature range of 1800 to 2100°C. Secondary ion mass spectrometry (SIMS) was used to identify the doping profiles, which showed very high aluminum concentration (5×1019 cm−3) near the surface and linearly graded boron profile up to several micrometers in depth. Hall-effect measurement was also employed to obtain the carrier concentration, which showed more than 1019 cm−3 carrier concentration at room temperature. Cathodoluminescence (CL) image clearly illustrated the locally diffused pattern. In addition, planar p-n diodes based upon this technique were fabricated and current-voltage (I-V) characteristics were measured. Excellent rectification property has been obtained. Built-in voltage of 2.9 V in the formed p-n junction was obtained by capacitance-voltage (C-V) measurement.

Type
Research Article
Copyright
Copyright © Materials Research Society 2001

Access options

Get access to the full version of this content by using one of the access options below. (Log in options will check for institutional or personal access. Content may require purchase if you do not have access.)

References

REFERENCES

1. Choyke, W. J. and Devaty, Robert P., SiC—The Power Semiconductor for the 21st Century: A Materials Perspective, Naval Research Reviews, Vol. 51, No. 1,Google Scholar
2. Dmitriev, V. A. and Spencer, M. G., SiC Fabrication Technology: Growth and Doping, Eds, Park, Y. S., SiC Materials and Devices, Vol.52, 1998.Google Scholar
3. Soloviev, S. I., Gao, Y., Khlebnikov, I. I. and Sudarshan, T. S., Selective Doping of 6H-SiC by Diffusion of Boron, Proceedings of the International Conference on Silicon Carbide and Related Materials-1999, North Carolina, USA, Eds, Carter, C. H., Devaty, R. P. and Rohrer, G. S..Google Scholar
4. Vodakov, Y. A. and Mokhov, E. N., in: Silicon Carbide—1973, Eds. Marshall, R. C., Faust, J. W., Univ. of South Carolina Press, Columbia, 1974 (p.508).Google Scholar
5. Ramungul, Nudjarin, Design and Characterization of 6H-SiC Devices for High-Power and High-Temperature Applications, Ph.D Thesis in Rensselaer Polytechnic Institute, Mar. 1998.Google Scholar
6. Jenny, J. R. and Skowronski, J. and Mitchel, W.C., et al, Deep Level Transient Spectroscopic and Hall Effect Investigation of the Position of the Vanadium Acceptor Level in 4H and 6H SiC, Appl. Phys. Lett., 68 (14), 1 April 1996.Google Scholar
7. Troffer, T., Schadt, M., Frank, T., Itoh, H., Pensl, G., Heindl, J., Strunk, H. P., Maier, M., Doping of SiC by Implantation of Boron and Aluminum, phys. Stat. Sol. (a) 162, 277 (1997).Google Scholar
8. Wirth, H., Panknin, D., and Skorupa, W., Efficient p-type doping of 6H-SiC: Flash-lamp annealing after aluminum implantation, Applied Phisics Letters, Vol.74, No. 7, 15 Feb.,1999.Google Scholar
9. Brezeanu, G., Badila, M., Tudor, B., Godignon, P., Millan, J., Locatelli, M. L., Chante, J. P., Lebedev, A., Savkina, N. S., Electrical Characteristics Modeling of Large Area Boron Compensated 6H-SiC pn Structures, Solid-State Electronics, 44 (2000).Google Scholar