Hostname: page-component-586b7cd67f-t7czq Total loading time: 0 Render date: 2024-11-23T11:42:17.026Z Has data issue: false hasContentIssue false

Properties of Au/Pb(Zr0.52Ti0.48)O3/ Bi4Ti3O12/p-Si Ferroelectric Memory Diodes

Published online by Cambridge University Press:  21 March 2011

Jun Yu
Affiliation:
Department of Electronic Science & Technology, Huazhong University of Science & Technology, Wuhan, 430074, China
Hua Wang
Affiliation:
Department of Electronic Science & Technology, Huazhong University of Science & Technology, Wuhan, 430074, China Department of Electron & Information, Guilin institute of Electronic Technology, Guilin, 541004, China
Xiaomin Dong
Affiliation:
Department of Electronic Science & Technology, Huazhong University of Science & Technology, Wuhan, 430074, China
Wenli Zhou
Affiliation:
Department of Electronic Science & Technology, Huazhong University of Science & Technology, Wuhan, 430074, China
Yunbo Wang
Affiliation:
Department of Electronic Science & Technology, Huazhong University of Science & Technology, Wuhan, 430074, China
Lili Zhu
Affiliation:
Department of Electronic Science & Technology, Huazhong University of Science & Technology, Wuhan, 430074, China
Get access

Abstract

A ferroelectric memory diodes that consists of Au/Pb(Zr0.52Ti0.48)O3/Bi4Ti3O12/p-Si multilayer configuration was fabricated by pulsed laser deposition (PLD) technique. The ferroelectric properties and the electrical characteristics of the ferroelectric film system were investigated. The polarization-voltage curve of Pb(Zr0.52Ti0.48)O3/Bi4Ti3O12 thin films system had an asymmetry hysteresis loop with Pr=20μC/cm2 and Ec=48 kV/cm, and the decay in remnant polarization was only 10% after 109 switching cycles. The C-V curve and the I-V curve showed memory effects derived from the ferroelectric polarization of PZT/BIT films. The current density was 6.7×10−8A/cm2 at a voltage of +4V, and the conductivity behavior is discussed. The results suggested that the growth of the BIT ferroelectric layer is helpful to good ferroelectric properties, fatigue and capacitance retention characteristics.

Type
Research Article
Copyright
Copyright © Materials Research Society 2001

Access options

Get access to the full version of this content by using one of the access options below. (Log in options will check for institutional or personal access. Content may require purchase if you do not have access.)

References

[1] Scott, J. F. and Araujo, C. A.. Ferroelectric Memories. Science, 1989: 246: 14001405.Google Scholar
[2] Sinharoy, S., Buhay, H., Lampe, D. R.et al. Integration of ferroelectric thin films into nonvolatile memories. J. Vac. Sci. Tech. 1992: A10 (4): 15541561.10.1116/1.578044Google Scholar
[3] Watanabe, Y., Tanamura, M., Matsumots, Y.. Memory retention and switching speed of ferroelectric field-effect in (Pb,La)(Ti,Zr)O3 / La2CuO4:Sr heterostructure. Jpn. J. Appl. Phys. 1996: 35(2B): 15641568.10.1143/JJAP.35.1564Google Scholar
[4] Tadahiko, H., Kazuhiro, T., Takeharu, N.. Formation of metal / ferroelectric / insulator / semiconductor structure with a CeO2 buffer layer. Jpn. J. Appl. Phys., 1994: 33(Pt1.9B): 52195222.Google Scholar
[5] Yu, Jun, Jianhong, Zhao, Zhou, Wenli, et al. Formation and characteristics of Pb(Zr,Ti)O3 field-effect transistor with a SiO2 buffer layer. Appl. Phys. Lett. 1997: 70(4): 490492.10.1063/1.118190Google Scholar
[6] Buhay, H., Sinharoy, S., Kasner, W. H.. Pulsed Laser Deposition and ferroelectric Characterization of Bismuth Titanate Films. Appl. Phys. Lett. 1991: 58(14): 14701472.10.1063/1.105200Google Scholar
[7] Wu, Y. S.. A new ferroelectric memory device, metal-ferroelectric-semiconductor transistor. IEEE Trans. electron. Dev., 1974: ED–21: 499504.Google Scholar
[8] Blom, P. W. M., Wolf, R. M., Cillessen, J. F. M., et al. Ferroelectric Schottky Diode. Phys. Rev. Lett. 1994: 73(15): 21072110.10.1103/PhysRevLett.73.2107Google Scholar
[9] Scott, J. F., Araujo, C. A., Melick, B. M.et al. Quantitative measurement of space charge effect in lead-zirconate-titanate memories. J. Appl. Phys. 1991: 70(1): 382386.10.1063/1.350286Google Scholar