Processing and Properties of Reaction Bonded Silicon Nitride Made from Laser Synthesized Silicon Powders
Published online by Cambridge University Press: 28 February 2011
Abstract
Laser synthesized silicon powders have been used to make reaction bonded silicon nitride samples. Maximum hardness (11.3 GNm−2), fracture toughness (3.6 MNm−3/2), pore size (Hg porosimetry 50–300Å radius) and strength (∼460 MNm−2) values reflect the superior microstructures that are observed. With anaerobic anhydrous processing, these powders nitride to completion in less than 7 hours at 1400°C.