Physical-Chemical Considerations for Semiconductor Room-Temperature Radiation Detectors
Published online by Cambridge University Press: 21 February 2011
Abstract
Physical properties of large band gap semiconductors such as: HgI2, CdTe, Cd0.8Zn0.2Te, CdSe, Cd0.7Zn0.3Se, GaAs, PbI2 and TlBr are briefly reviewed and discussed in terms of their use as room temperature operating x-ray and gamma ray radiation detectors. It is shown that HgI2 which has the largest drift length for holes, λ=μτE i.e., the product of the mobility μh, life time τh and the electrical field E, is at present the leading material, being followed by the newly developed Cd0.8Zn0.2Te. Chemical defects in HgI2 were enhanced by doping the material with aliphatic, aromatic and oxyhydrocarbons as well as with excess Hg and I2 and the increase in unit cell parameter was studied as a function of the amount of dopant. The value of τ was measured as a function of dopant concentration and it was found that Hg doping causes the most severe trapping defects. Low temperature studies of τh down to 170K allowed the identification of the trapping energy levels and concentration of electrically active defects. Shallow traps of 0.13-0.18 eV stemming from deviation from stoichiometry of H-gI2 were found to be in the ppm level whereas deeper traps of 0.4-0.5 eV stemming from hydrocarbons were found to be in the ppb level. It is concluded that only extensive research on the physical, chemical and structural defects correlated with improved crystal growth and device fabrication methods, would lead, in the future, to improvements in λh also of the other large Eg semiconductor detector materials.
- Type
- Research Article
- Information
- Copyright
- Copyright © Materials Research Society 1993
References
REFERENCES
- 2
- Cited by