Article contents
Optimization of a Tin/TiSi2 p+ Diffusion Barrier Process
Published online by Cambridge University Press: 25 February 2011
Abstract
The TiN/TiSi2 structure, formed by rapid thermal nitridation of a spatter-deposited titanium film, has been demonstrated to be effective as a diffusion barrier and as a low resistance contact material for VLSI submicron metallization. An optimization experiment, designed using the RS/Discover software package, was used to identify a metallization process that minimized p+ resistance as well as maximized barrier capability. Source/drain implant doses, as-deposited titanium film thickness, and rapid thermal processing parameters were the factors varied in the experiment. Of particular significance is a comparison of the effects of a two-step versus one-step rapid thermal anneal on control of the TiN/TiSi2 thickness ratio. A TiN layer of sufficient thickness for barrier integrity and adequate consumption of implant damage in the formation of the TiSi2 layer are desired. Electrical and thermal stability measuremints of the resultant AlSiCu/TiN/TiSi2 p+ contact system are presented.
- Type
- Research Article
- Information
- Copyright
- Copyright © Materials Research Society 1989
References
REFERENCES
- 3
- Cited by