Nanostructures from Hydrogen and Helium Implantation of Aluminum

Published online by Cambridge University Press:  01 February 2011

Markus D. Ong
Affiliation:
[email protected], Sandia National Laboratories, Energy Nanomaterials, Livermore, California, United States
Nancy Yang
Affiliation:
[email protected], Sandia National Laboratories, Energy Nanomaterials, Livermore, California, United States
Ryan J. Depuit
Affiliation:
[email protected], University of California, Santa Barbara, Chemical Engineering, Santa Barbara, California, United States
Bruce R. McWatters
Affiliation:
[email protected], Sandia National Laboratories, Radiation-Solid Interactions, Albuquerque, New Mexico, United States
Rion A. Causey
Affiliation:
[email protected], Sandia National Laboratories, Energy Nanomaterials, Livermore, California, United States
Get access

Abstract

This study investigates a pathway to nanoporous structures created by hydrogen and helium implantation in aluminum. Previous experiments for fusion applications have indicated that hydrogen and helium ion implantations are capable of producing bicontinuous nanoporous structures in a variety of metals. This study focuses specifically on implantations of hydrogen and helium ions at 25 keV in aluminum. The hydrogen and helium systems result in remarkably different nanostructures of aluminum at the surface. Scanning electron microscopy, focused ion beam, and transmission electron microscopy show that both implantations result in porosity that persists approximately 200 nm deep. However, hydrogen implantations tend to produce larger and more irregular voids that preferentially reside at defects. Implantations of helium at a fluence of 1018 cm-2 produce much smaller porosity on the order of 10 nm that is regular and creates a bicontinuous structure in the porous region. The primary difference driving the formation of the contrasting structures is likely the relatively high mobility of hydrogen and the ability of hydrogen to form alanes that are capable of desorbing and etching Al (111) faces.

Type
Research Article
Copyright
Copyright © Materials Research Society 2010

Access options

Get access to the full version of this content by using one of the access options below. (Log in options will check for institutional or personal access. Content may require purchase if you do not have access.)

References

1 Conway, B.E. Electrochemical Supercapacitors. (Kluwer Academic/Plenum Publishers, New York, 1999).Google Scholar
2 Baldwin, M.J. and Doerner, R.P. Nucl. Fusion 48 (3), 5 (2008).Google Scholar
3 Wilson, K.L. and Thomas, G.J. J. Nucl. Mater. 63 (1), 266 (1976).Google Scholar
4 Chernikov, V.N. Alimov, V.K. Markin, A.V. Gorodetsky, A.E. Kanashenko, S.L. Zakharov, A.P., and Kupriyanov, I.B. J. Nucl. Mater. 233, 860 (1995).Google Scholar
5 Biener, J. Hodge, A.M. Hayes, J.R. Volkert, C.A. Zepeda-Ruiz, L.A., Hamza, A.V. and Abraham, F.F., Nano Lett. 6 (10), 2379 (2006).Google Scholar
6 Cattarin, S. Kramer, D. Lui, A. and Musiani, M.M. J. Phys. Chem. C 111 (34), 12643 (2007).Google Scholar
7 Shin, H.J. Ko, C.H. and Ryoo, R. J. Mater. Chem. 11 (2), 260 (2001).Google Scholar
8 Kang, H. Jun, Y. Park, J.I. Lee, K.B. and Cheon, J. Chem. Mater. 12 (12), 3530 (2000).Google Scholar
9 Yamauchi, Y. Momma, T. Yokoshima, T. Kuroda, K. and Osaka, T. J. Mater. Chem. 15 (20), 1987 (2005).Google Scholar
10 Attard, G.S. Bartlett, P.N. Coleman, N.R.B. Elliott, J.M. Owen, J.R. and Wang, J.H. Science 278 (5339), 838 (1997).Google Scholar
11 Robinson, D.B. Fares, S.J. Ong, M.D. Arslan, I. Langham, M.E. Tran, K. L. and Clift, W.M. Int. J. Hydrogen Energy 34 (13), 5585 (2009).Google Scholar
12 Stumpf, R. , R. and Scheffler, M. Phys. Rev. B53 (8), 4958 (1996).Google Scholar
13 Go, E.P. Thuermer, K. and Reutt-Robey, J.E., Surface Science 437 (3), 377 (1999).Google Scholar