Hostname: page-component-586b7cd67f-2brh9 Total loading time: 0 Render date: 2024-11-26T15:43:01.314Z Has data issue: false hasContentIssue false

Material Reliability and Integration Issues of Polyimide and Benzocyclobutene Interlayer Dielectric Materials

Published online by Cambridge University Press:  01 February 2011

Parshuram B. Zantye
Affiliation:
Department of Mechanical Engineering, Nanomaterials & Nanomanufacturing Research Center, University of South Florida, Tampa, Florida-33620
Ashok Kumar
Affiliation:
Department of Mechanical Engineering, Nanomaterials & Nanomanufacturing Research Center, University of South Florida, Tampa, Florida-33620
R. Gopalkrishnan
Affiliation:
Institute of Microelectronics, Science Park II, Singapore, 117685
S. Balakumar
Affiliation:
Institute of Microelectronics, Science Park II, Singapore, 117685
Get access

Abstract

The constant push for decreasing the Resistance-Capacitance (RC) delay has led to the implementation of Multilevel Metallization (MLM) scheme for interconnect wiring, Cu as the wiring material and low ê materials as Interlayer Dielectric (ILD). Polymeric materials are being explored to replace SiO2 based ILD materials in the next generation ICs. Several reliability and integration challenges arise during integration of the candidate polymeric ILD when they are subjected to planarization by Chemical Mechanical Polishing (CMP). In this research, we have performed a comparative study of certain candidate low ê materials: 1) undoped SiO2 (standard), 2) Polyimide and 3) Benzocyclobutene (BCB). We have studied the impact of reduction in dielectric constant on the mechanical and tribological properties, and the CMP performance of these ILD materials. The adverse effect of shear and mechanical abrasion due to decreased mechanical properties of the low ê materials induced numerous defects during CMP.

Type
Research Article
Copyright
Copyright © Materials Research Society 2005

Access options

Get access to the full version of this content by using one of the access options below. (Log in options will check for institutional or personal access. Content may require purchase if you do not have access.)

References

1. Zantye, P. B., Kumar, A., Sikder, A., Mat. Sci. Eng. R, 45, 3-6, 89, (2004).Google Scholar
2. Ryan, J.G., Geffken, RM, Poulin, NR, and Paraszczak, JR, IBM J. Res. Dev., 39, 371, (1995).Google Scholar
3. Abell, T., Shamiryan, D., Iacopi, F., and Maex, K., Mat. Today, 7, 1, 34, (2004).Google Scholar
4. Kim, Y.H., M. S.Hwang, Kim, H. J., Kim, J. Y. and Lee, Y., J. Appl. Phys., 90, 3367, (2001).Google Scholar
5. Oliver, W.C. and Pharr, G.M., J. Mater. Res., 7, 1564, (1992).Google Scholar
6. A Sikder, K., Wood, J., Giglo, F., Kumar, A. and Anthony, J. M., J. of Electron. Mater., 30, 1522, (2001).Google Scholar
7. Cook, L.M., J. Non-Cryst. Solids, 120, 152, (1990).Google Scholar
8. Borst, C. L., Gill, WN and Gutmann, RJ, J. Electrochem. Soc., 146, 11, 4309 (1999).Google Scholar
9. Philipossian, A. and Olsen, S., J. Electrochem. Soc, 151, 6,G 436, (2004).Google Scholar
10. Sikder, A.K., Zantye, P.B., Thagella, S. and Kumar, A., Proceedings of 8th CMPMIC Conference, pp. 120, (2003).Google Scholar
11. Zantye, P. B., Kumar, A., Dallas, W., Ostapenko, S. and Sikder, A.K., Submitted to the J. Vac. Sci Tech. B, (2005).Google Scholar
12. Qin, K., Moudgi, B., Park, C.W, Thin Solid Films, 446, 2, 277, (2004).Google Scholar