Article contents
Low Temperature Kinetics for the Growth and Decay of Band-Tallcarriers and Dangling Bonds in Hydrogenated Amorphous Silicon
Published online by Cambridge University Press: 15 February 2011
Abstract
In hydrogenated amorphous silicon (a-Si:H), the kinetics of the light induced production of silicon dangling bonds and long-lived band-tail electrons and holes has been measured at temperatures between 65 and 340 K using light induced electron spin resonance (LESR). Below about 150 K the measurement of Si dangling bonds is masked by the accumulation of long-lived band-tail carriers. The kinetics of the growth and decay of these long-lived, trapped band-tail carriers consists of very fast components (τ < ms) and very long components (τ > h). Optical quenching of these long-lived carriers is not efficient at quenching energies of 0.6 eV. Afler removal of these long-lived band tail carriers by annealing at about 250 K we find that the total production of silicon dangling bonds at 65 K after 10 h of illumination is about a factor of five less than at 340 K. The dangling bond production resulting from 10 h of illumination is well fit to an underlying mechanism that, if thermally activated, exhibits an activation energy of approximately 10 meV.
- Type
- Research Article
- Information
- Copyright
- Copyright © Materials Research Society 1999
References
- 4
- Cited by