Low Temperature Deposition of High Dielectric Constant Thin Films for Decoupling Capacitor Applications

Published online by Cambridge University Press:  25 February 2011

P. Li
Affiliation:
Center for Integrated Electronics and Physics Department, Rensselaer Polytechnic Institute, Troy, NY 12180
B. Gittleman
Affiliation:
Center for Integrated Electronics and Physics Department, Rensselaer Polytechnic Institute, Troy, NY 12180
T.-M. Lu
Affiliation:
Center for Integrated Electronics and Physics Department, Rensselaer Polytechnic Institute, Troy, NY 12180
Get access

Abstract

High dielectric constant thin films for packaging applications were studied. Compared with polycrystalline or epitaxial ferroelectric thin films amorphous ferroelectric films are a promising alternative because of their ease of processing and low leakage current. Reactive Partially Ionized Beam deposition (RPIB) offers a new approach to deposit high dielectric constant films at a low substrate temperature. As an example, the growth of amorphous BaTiOs thin films using RPIB deposition is described. The films were characterized in terms of dielectric constant and leakage current. The annealing effects on the film properties are also discussed.

Type
Research Article
Copyright
Copyright © Materials Research Society 1991

Access options

Get access to the full version of this content by using one of the access options below. (Log in options will check for institutional or personal access. Content may require purchase if you do not have access.)

References

REFERENCES

[1] Nakagawa, T., Yamaguchi, J., Okuyama, M., and Hamakawa, Y., Jap. J. Appl. Phys. 21, L655 (1982).Google Scholar
[2] Adachi, M., Matsuzaki, T., Yamada, T., Shiosaki, T. and Kawabata, A., Jap. J. Appl. Phys. 26, 550, (1987).Google Scholar
[3] Castellano, R. N., and Feinstein, L. G., J. Appl. Phys. 50, 4406, (1979).Google Scholar
[4] lijima, K., Takayama, R., Tomita, Y., and Ueda, I., J. Appl. Phys. 60, 2914, (1986).Google Scholar
[5] Adachi, H., Mitsuyu, T., Yamazaki, O., and Wasa, K., J. Appl. Phys. 60, 736, (1986).Google Scholar
[6] Okada, A., J. Appl. Phys. 49, 4495, (1978).Google Scholar
[7] lijima, K., Terashima, T., Yamamoto, K., Hirata, K., and Bando, Y., Appl. Phys. Lett. 56, 527, (1990).Google Scholar
[8] Parker, L. H. and A Tasch, l. F., IEEE Circuits and Devices Magazine 6, 17, (1990).Google Scholar
[9] Gerson, R., J. Appl. Phys. 31, 188, (1960).Google Scholar
[10] Miller, C. A., Brit. J. Appl. Phys. 18, 1689, (1967).Google Scholar
[11] Kulcsar, F., J. Am. Ceram. Soc. 42, 343, (1959).Google Scholar
[12] Carrano, J., Sudhama, C., Lee, J., Tasch, Al, and Miller, W., IEEE IEDM Tech. Digest p10.2.1 (1989).Google Scholar
[13] Sreenivas, K. and Mansingh, A., J. Appl. Phys. 62, 4475, (1987).Google Scholar
[14] Krupanidhi, S. B., Maffei, N., Sayer, M., and El-Assal, K., J. Appl. Phys. 54, 1983.Google Scholar
[15] Olson, J. C. and Stevison, D. F., Ferroelectrics 37, 685, (1981).Google Scholar
[16] Iijima, T. Terashima, Yamamoto, K., Hirta, K., and Bando, Y., Appl. Phys. Lett. 56, 527, (1990).Google Scholar
[17] Dharmadhikari, V. S. and Grannemann, W. W., J. Appl. Phys. 53, 8988, (1982).Google Scholar
[18] Panitz, J. K. G. and Hu, C.-C., J. Vac. Sci. Technol. 16, (2), 315 (1979).Google Scholar
[19] McClure, D. J. and Crowe, J. R., J. Vac. Sci. Technol. 16, (2), 311 (1979).Google Scholar
[20] Pratt, I. H. and Firestone, S., J. Vac. Sci. Technol. 8, 256, (1970).Google Scholar
[21] Muller, E. K., Nicholson, B. J. and Francombe, M. H., Electrochem. Tech. 1, 156, (1963).Google Scholar
[22] Shintani, Y. and Tada, O., J. Appl. Phys. 41, 2376, (1970).Google Scholar
[23] Wohlecke, M., Marrello, V. and Onton, A., J. Appl. Phys. 48, 1748, (1977).Google Scholar
[24] Rose, T. L., Kelliher, E. M., Scoville, A. N., and Stone, S. E., J. Appl. Phys. 55, 3706, (1984).Google Scholar
[25] Li, P. and Lu, T.-M., Appl. Phys. Lett. 57, 2336, (1990). (1990).Google Scholar
[26] Wong, J. and Lu, T.-M., and Mehta, S., J. Vac. Sci. Technol. B3, (1985).Google Scholar
[27] Rossnagel, S. M., and Cuomo, J. J., MRS Bulletin 12, 48, (1987).Google Scholar
[28] Takagi, T., Ionized-Cluster Beam Deposition and Epitaxy, Noyes Data Corporation and Noyes Publications, NJ, (1988) 78.Google Scholar
[29] Isobe, C. and Saitoh, M., Appl. Phys. Lett. 56, 907, (1990).Google Scholar