Hostname: page-component-78c5997874-v9fdk Total loading time: 0 Render date: 2024-11-05T12:09:13.613Z Has data issue: false hasContentIssue false

Kinetic Lattice Monte Carlo Simulations of Cascade Aging in Iron and Dilute Iron-Copper Alloys

Published online by Cambridge University Press:  10 February 2011

B. D. Wirth
Affiliation:
Dept. of Mechanical and Environmental Engineering, University of California, Santa Barbara, CA 93106
G. R. Odette
Affiliation:
Dept. of Mechanical and Environmental Engineering, University of California, Santa Barbara, CA 93106
Get access

Abstract

Neutron hardening and embrittlement of pressure vessel steels is due to a high density of nm scale features, including copper-manganese-nickel rich precipitates and what are generally believed to be defect cluster-solute complexes. It has been postulated that the sub nanometer defect cluster-solute complexes form directly in displacement cascades. Cluster-complexes that are thermally unstable mediate the effect of flux on embrittlement kinetics. Larger cluster-complexes, that are relatively thermally stable for irradiation times up to 1 Gs, cause embrittlement in low copper steels. Robust characterization of these two types of so-called matrix defects has been an elusive goal. In this work, Kinetic Lattice Monte Carlo (KLMC) simulations of the long term evolution of the vacancy-rich cascade core regions were carried out for both pure iron and dilute iron-copper alloys at the nominal irradiation temperature of 563°K up to times when the vacancy clusters completely dissolve. Energetics were based on lattice embedded atom method potentials. Special time scaling and pulse annealing techniques were used to deal with the enormous range of inherent time scales involved, viz., rapid free vacancy jumps to slow emission from large complexes. Three-dimensional clusters rapidly form, containing a wide range of vacancies, as well as copper atoms in alloys. Small complexes are very mobile and growth takes place primarily by coalescence. The vacancy clusters ultimately dissolve at times from less than 0.1 to more than 100 MS. These simulations support the hypotheses that cascade cluster-complexes constitute both thermally stable and unstable matrix defect features.

Type
Research Article
Copyright
Copyright © Materials Research Society 1999

Access options

Get access to the full version of this content by using one of the access options below. (Log in options will check for institutional or personal access. Content may require purchase if you do not have access.)

References

1. Seeger, A., Proc. 2nd UN Int. Conf. on Peaceful Uses of Atomic Energy, Geneva, Vol. 6, United Nations, New York (1958) 20 Google Scholar
2. Robinson, M. T., J. Nucl. Mat. 216 (1994) 1.Google Scholar
3. Stoller, R. E., MRS Soc. Symp. Proc. 373 (1995) 21.Google Scholar
4. Calder, A. F. and Bacon, D. J., J. Nucl. Mat. 207 (1993) 25.Google Scholar
5. Odette, G. R., MRS Soc. Symp. Proc., 373 (1995) 137.Google Scholar
6. Odette, G. R. and Wirth, B. D., J. Nucl. Mater. 251 (1997) 157.Google Scholar
7. Wirth, B. D., Odette, G. R., Maroudas, D., and Lucas, G. E., J. Nucl. Mat. 244 (1997) 185.Google Scholar
8. Wirth, B. D., Odette, G. R., Maroudas, D., and Lucas, G. E., MRS Soc. Symp. Proc. 504 (1998), in press.Google Scholar
9. Wirth, B. D., On the Character of Nano-scale Features in Reactor Pressure Vessel Steels Under Neutron Irradiation, Ph.D. Dissertation, University of California, Santa Barbara (1998).Google Scholar
10. Jenkins, M. L., Kirk, M. A. and Phythian, W. J., J. Nucl. Matrl. 205 (1993) 16.Google Scholar
11. Finnis, M. W. and Sinclair, J. E., Phil. Mag. A 50 (1) (1984) 45.Google Scholar
12. Ackland, G. J., Tichy, G. I., Vitek, V., and Finnis, M. W., Phil. Mag. A 56 (1987) 735.Google Scholar
13. Wirth, B. D. and Odette, G. R., MRS Soc. Symp. Proc. 481 (1998), in press.Google Scholar
14. Moslang, A., Albert, E., Recknagel, E. and Weidinger, A., Hyperfine Interactions, 15/16 (1983) 409.Google Scholar
15. Odette, G. R., Neutron Irradiation Effects in Reactor Pressure Vessel Steels and Weldments, IAEA IWG-LMNPP-98/3, International Atomic Energy Agency, Vienna (1998) 438.Google Scholar
16. Mader, E. V., Kinetics of Irradiation Embrittlement and the Post-Irradiation Annealing of Nuclear Reactor Pressure Vessel Steels, Ph.D. Dissertation, University of California Santa Barbara (1995).Google Scholar