Hostname: page-component-78c5997874-4rdpn Total loading time: 0 Render date: 2024-11-17T19:12:36.716Z Has data issue: false hasContentIssue false

Intrinsic Stress of Pecvd Silicon Oxynitride Films Deposited in a Hot-Wall Reactor

Published online by Cambridge University Press:  16 February 2011

K. Aite
Affiliation:
University of Twente, Integrated Circuits Technology and Electronics Lab., P.O.Box 217, 7500 AE, Enschede, The Netherlands.
R. Koekoek
Affiliation:
Tempress B.V., Marconistraat 14, 7903 AG Hoogeveen, The Netherlands.
Get access

Abstract

Plasma enhanced chemical vapor deposited ( PECVD ) silicon oxynitride films with refractive indices varying from 1.65 to 1.85 have been deposited in a hot-wall reactor using a SiH4/NH3/N2O gas mixture. A systematic investigation of the variation of the intrinsic stress of the deposited films with the parameters of deposition and the properties of the films, has been carried out. Our results show that silicon oxynitride films deposited in optimal conditions can support annealing temperatures of 900°C without cracking. The mechanical stresses in the films were determined by the Newton's fringes technique and a surface profiler. The film thickness was measured by ellipsometry at a wavelength of 632.8 nm. Fourier transform infrared spectroscopy ( FTIR ) was used to measure the hydrogen content of the films. The composition of the silicon oxynitride films was determined by Auger electron spectroscopy ( AES ) and Rutherford backscattering spectrometry ( RBS ).

Type
Research Article
Copyright
Copyright © Materials Research Society 1990

Access options

Get access to the full version of this content by using one of the access options below. (Log in options will check for institutional or personal access. Content may require purchase if you do not have access.)

References

REFERENCES

[1] Claassen, W.A.P., Valkenburg, W.G.J.N., Willemsen, M.F.C., and Wijgert, W.M.v.d., J. Electrochem. Soc., 132, p.893, April 1985.Google Scholar
[2] Aite, K., Koekoek, R., Holleman, J. and Middelhoek, J., Journal de Physique, C5, Supplement to No.5, 50, pp. 323–31, May 1989.Google Scholar
[3] Koyama, K., Takasaki, K., Maeda, M., and Takagi, L.M., Abstract 301, p. 738, The Electrochem. Soc. Extended Abstracts, 81–2, Denver, Colorado, 11–6 Oct. 1981.Google Scholar
[4] Claassen, W.A.P. and Kuiper, A.E.T., Proc. of the 7th Intl. Symp. on Plasma Chemistry, Eindhoven, The Netherlands, edited by Timmermans, C.J., 1, p. 130, July 1–5, 1985.Google Scholar
[5] Lanford, W.A. and Rand, M.J., J. Electrochem. Soc., 49, p. 2472, 1978.Google Scholar
[6] Aite, K., Holleman, J., Middelhoek, J. and Koekoek, R., Mat. Res. Soc. Symp. Proc., 130, pp. 347–53, (1989) (and references therein).Google Scholar
[7] Flamm, D.L. and Herb, G.K., in “Plasma Etching: An Introduction” Edited by Manos, D.M. and Flamm, D.L., p.36, Academic Press, Inc., (1989).Google Scholar
[8] Claassen, W.A.Y.P., Pol, H.A.J. Th.v.d., Goemans, A.H. and Kuiper, A.E.T., J. Electrochem. Soc., 133(7), pp.1458–63, July 1986.Google Scholar