Hostname: page-component-586b7cd67f-l7hp2 Total loading time: 0 Render date: 2024-11-29T07:48:56.715Z Has data issue: false hasContentIssue false

Interaction of A12O3-CAPPED Au/Zn/Au and Au/Te/Au Contacts With (001)GaAs Substrates

Published online by Cambridge University Press:  25 February 2011

X. W. Lin
Affiliation:
Materials Science Division, Lawrence Berkeley Laboratory, University of California, Berkeley, CA 94720, U.S.A
Z. Liliental-Weber
Affiliation:
Materials Science Division, Lawrence Berkeley Laboratory, University of California, Berkeley, CA 94720, U.S.A
J. Washburn
Affiliation:
Materials Science Division, Lawrence Berkeley Laboratory, University of California, Berkeley, CA 94720, U.S.A
A. Piotrowska
Affiliation:
Institute of Electronic Technology, Al. Lotnikow 46, 02–668 Warsaw, Poland
E. Kaminska
Affiliation:
Institute of Electronic Technology, Al. Lotnikow 46, 02–668 Warsaw, Poland
Get access

Abstract

HREM,TEM, and EDX were employed to study the cross sections of Au/Zn/Au and Au/Te/Au contacts to [001]-oriented GaAs substrates. The metal contacts fabricated by sequential vapor deposition were capped with an A12O3 thin film to form a closed system when subjected to a 420°C anneal for 3 min. For an as-deposited Au/Zn/Au/GaAs specimen, Zn was found to react with Au to form ordered phases of Au3Zn. These phases were found to be stable upon annealing. The interface between the annealed metallization and GaAs exhibited the same degree of uniformity and planarity as that of the as-deposited specimen. For a Au/Te/Au/GaAs specimen, annealing resulted in epitaxial growth of Ga2Te3 grains, forming a basically flat interface with GaAs, while Au single-crystal grains were found to protrude rather extensively into GaAs to form a facetted interface with the substrate.

Type
Research Article
Copyright
Copyright © Materials Research Society 1992

Access options

Get access to the full version of this content by using one of the access options below. (Log in options will check for institutional or personal access. Content may require purchase if you do not have access.)

References

REFErences

1. Barcz, A. J., Kaminska, E., and Piotrowska, A., Thin Solid Films 149, 251 (1987).CrossRefGoogle Scholar
2. Piotrowska, A., Kaminska, E., Guziewicz, M., Veresegyhazy, R., Mojzes, I., and Pecz, B., Acta Physica Polonica, 80 (3), 457 (1991).CrossRefGoogle Scholar
3. Yoshiie, T., Bauer, C. L., and Milnes, A. G., Thin Solid Films 111, 149 (1984).CrossRefGoogle Scholar
4. Liliental-Weber, Z., Washburn, J., Newman, N., Spicer, W. E., and Weber, E. R., Appl. Phys. Lett. 49, 1514 (1986).CrossRefGoogle Scholar
5. to be published.Google Scholar
6. Sheng, T. T., in “Analytical Techniques For Thin Films” edited by Tu, K. N. and Rosenberg, R. (Academic Press, 1988), pp. 251 - 296.Google Scholar
7. Wilkens, M. and Schubert, K., Metallkde, Z..49, 633 (1958).Google Scholar
8. Iwasaki, H., J. Phys. Soc. Japan 17, 1620 (1962).CrossRefGoogle Scholar
9. Zeng, X. F. and Chung, D. D. L., Thin Solid Films 93, 207 (1982).CrossRefGoogle Scholar
10. Braslau, N., J. Vac. Sci. Technol. 19, 803 (1981).CrossRefGoogle Scholar