Impact of Metal Contamination of 7.0nm Gate Oxides on Various Substrate Materials

Published online by Cambridge University Press:  10 February 2011

S. Saito
Affiliation:
ULSI Device Develop. Labs., NEC, 1120 Shimokuzawa, Sagamihara, 229–11 JAPAN
K. Hamada
Affiliation:
ULSI Device Develop. Labs., NEC, 1120 Shimokuzawa, Sagamihara, 229–11 JAPAN
D. J. Eaglesham
Affiliation:
Bell Labs., Lucent Technologies, 600 Mountain Avenue, Murray hill, NJ 07974
Y. Shiramizu
Affiliation:
ULSI Device Develop. Labs., NEC, 1120 Shimokuzawa, Sagamihara, 229–11 JAPAN
J. L. Benton
Affiliation:
Bell Labs., Lucent Technologies, 600 Mountain Avenue, Murray hill, NJ 07974
H. Kitajima
Affiliation:
ULSI Device Develop. Labs., NEC, 1120 Shimokuzawa, Sagamihara, 229–11 JAPAN
S. D. C. Jacobson
Affiliation:
Bell Labs., Lucent Technologies, 600 Mountain Avenue, Murray hill, NJ 07974
J. M. Poate
Affiliation:
Bell Labs., Lucent Technologies, 600 Mountain Avenue, Murray hill, NJ 07974
Get access

Abstract

Metal contamination level will be decreased in order to maintain a device reliability according to device size reduction. Metal contamination from various processes are surveyed. The influence of metal contamination for 7–15nm thick gate oxides is discussed in order to clarify the critical concentration to gate oxides. NIG(Non Intrinsic Gettering) substrates are used in a worst case for gettering. Fe contamination with 4×1010 cm-2 strongly affects the TDDM characteristics, although there is no serious influence in the breakdown voltage even at the concentration of 5×1011 cm-2. The same tendency is observed for Cu contaminant and the critical concentration for TDDB characteristics is around 3×1011 cm-2. High energy B implantation is carried out to form gettering sites near device region. Breakdown voltage and TDDB characteristics are almost the same as epitaxial substrates at Fe concentration up to 1×1012 cm-2. Detailed examination such as SIMS, C-t and DLTS measurements is also supported the effectiveness in high energy gettering.

Type
Research Article
Copyright
Copyright © Materials Research Society 1997

Access options

Get access to the full version of this content by using one of the access options below. (Log in options will check for institutional or personal access. Content may require purchase if you do not have access.)

References

REFERENCES

1. Shiramizu, Y. and Kitajima, H., Extended Abstracts of the 1995 Conference on Solid State Devices and Materials, p273 (1995)Google Scholar
2. Ryuta, J., Yoshimi, T.,, Kondo, H., Okuda, H. and Shimanuki, Y., Jpn J. Appl. Phys. 31, p2338 (1992)Google Scholar
3. Shiramizu, Y., Tanaka, M., Yamazaki, S., Nakamori, M., Aoto, N. and Kitajima, H., Extended Abstracts of the 1996 Conference on Solid State Devices and Materials, p362 (1996)Google Scholar
4. Benton, J.L., Stolk, P.A., Eaglesham, D.J., Jacobson, D.C., Cheng, J.Y., Poate, J.M., Myers, S.M. and Haynes, T.E., J. Electrochem. Soc., 143, p1406 (1996)Google Scholar
5. Hamada, K., Eaglesham, D.J., Hayashi, T., Poate, J.M. and Saito, S., Extended Abstracts of the 1996 Conference on Solid State Devices and Materials, p854 (1996)Google Scholar