Fracture Behavior of Micro-Sized Ni-P Amorphous Alloy Specimens

Published online by Cambridge University Press:  10 February 2011

Y. Ichikawa
Affiliation:
Precision and Intelligence Laboratory, Tokyo Institute of Technology 4259 Nagatsuta-cho, Midori-ku, Yokohama 226-8503, Japan, [email protected]
S. Maekawa
Affiliation:
Precision and Intelligence Laboratory, Tokyo Institute of Technology 4259 Nagatsuta-cho, Midori-ku, Yokohama 226-8503, Japan, [email protected]
K. Takashima
Affiliation:
Precision and Intelligence Laboratory, Tokyo Institute of Technology 4259 Nagatsuta-cho, Midori-ku, Yokohama 226-8503, Japan, [email protected]
M. Shimojo
Affiliation:
Precision and Intelligence Laboratory, Tokyo Institute of Technology 4259 Nagatsuta-cho, Midori-ku, Yokohama 226-8503, Japan, [email protected]
Y. Higo
Affiliation:
Precision and Intelligence Laboratory, Tokyo Institute of Technology 4259 Nagatsuta-cho, Midori-ku, Yokohama 226-8503, Japan, [email protected]
M. V. Swain
Affiliation:
Biomaterials Science Research Unit, University of Sydney, Australian Technology Park Eveleigh, NSW 1490, Australia
Get access

Abstract

Fracture behavior of micro-sized Ni-P Amorphous alloy specimens has been investigated using a newly developed mechanical testing machine. Specimens with dimensions of 10 × 12 × 50 μm were prepared by focused ion beam machining. Two types of specimens with different crack geometries were prepared. One specimen has a notch with root radius is 0.25 μtm and the other has a fatigue pre-crack. The shapes of the loaddisplacement curves are different for each type of specimen. The fracture strength of the specimens with a notch is higher than that with a fatigue pre-crack and the fracture surfaces of the specimens are also different for each type of specimen. This may be due to the difference in stress concentration at the crack (notch) tip, and indicates that even a notch with a root radius of 0.25 μm is not able to be regarded as a crack for micro-sized specimens. Therefore, the introduction of a fatigue pre-crack is essential for the evaluation of fracture toughness for such micro-sized specimens.

Type
Research Article
Copyright
Copyright © Materials Research Society 2000

Access options

Get access to the full version of this content by using one of the access options below. (Log in options will check for institutional or personal access. Content may require purchase if you do not have access.)

References

1. Sato, K., Yoshioka, T., Ando, T., Shikida, M. and Kawabata, T., Sensors & Actuators A: Physical 70, 148 (1998)Google Scholar
2. Sharpe, W.N. Jr, Brown, S., Johnson, G.C., Knauss, W., in Microelectromechanics Structures for Materials Research, edited by Brown, S., Gilbert, J., Gruckel, H., Howe, R., Johnson, G., Krulevitch, P., Muhlstein, C., (Mat. Res. Soc. Proc. 518, Piltsburgh, PA, 1998) pp.5765.Google Scholar
3. Ballarini, R., Muller, R.L., Yin, Y., Kahn, H., Sempen, S. and Heuer, A.H., J. Mat. Res. 12, 915 (1997)Google Scholar
4. Craft, O., Schwaiger, R. and Nix, W.D., in Microelectromechanics Structures for Materials Research, edited by Brown, S., Gilbert, J., Gruckel, H., Howe, R., Johnson, G., Krulevitch, P., Muhlstein, C., (Mat. Res. Soc. Proc. 518, Piltsburgh, PA, 1998) pp. 3944.Google Scholar
5. Takashima, K., Kimura, T., Shimojo, M., Higo, Y., Sugiura, S., Pfister, B. and Swain, M. V., 7th Int. Fatigue Cong., edited by Wu, X. R. and Wang, Z. G. (Higher Education Press, Cradley Heath, UK, 1999), pp. 18711876.Google Scholar
6. Takashima, K., Maekawa, S., Shimojo, M., Higo, Y., Sugiura, S. and Swain, M. V., in Proc. 1999 Annual Meeting of JSME/MMD, edited by Ohtani, R. (Japan Soc. of Mechanical Eng., Tokyo, Japan, 1999), pp 6364 (in Japanese).Google Scholar
7. Maekawa, S., Takashima, K., Shimojo, M., Higo, Y., Sugiura, S., Pfister, B. and Swain, M. V., Microprocesses and Nanotechnology Conf., edited by Horiike, Y. (The Japan Society of Applied Physics, Tokyo, Japan, 1999), pp. 132133.Google Scholar
8. Maekawa, S., Takashima, K., Shimojo, M., Higo, Y., Sugiura, S. and Swain, M. V., in Proc. 1999 Annual Meeting of JSME/MMD, edited by Ohtani, R. (Japan Soc. of Mechanical Eng., Tokyo, Japan, 1999), pp 6768 (in Japanese).Google Scholar
9. Davis, L.A., J. Mater. Sci. 10, 1557 (1975)10.1007/BF01031856Google Scholar
10. Ewalds, H.L. and Wanhill, R.J.H. in Fractures Mechanics. (E.Amold, Kent, UK. 1991)p.49 Google Scholar