Hostname: page-component-cd9895bd7-gbm5v Total loading time: 0 Render date: 2024-12-27T02:30:35.776Z Has data issue: false hasContentIssue false

Evolution of Antiphase Domains and γ Lamellae in Ti-39at%Al Single Crystals

Published online by Cambridge University Press:  26 February 2011

Yuichiro Koizumi
Affiliation:
[email protected], Osaka University, Adaptive Machine Systems, 2-1, Yamadaoka, Suita, 565-0871, Japan, 81-6-6879-7434, 81-6-6879-4174
Kazuki Iwamoto
Affiliation:
[email protected], Osaka University, Adaptive Machine Systems, 2-1, Yamadaoka, Suita, 565-0871, Japan
Takayuki Tanaka
Affiliation:
[email protected], Osaka University, Adaptive Machine Systems, 2-1, Yamadaoka, Suita, 565-0871, Japan
Yoritoshi Minamino
Affiliation:
[email protected], Osaka University, Adaptive Machine Systems, 2-1, Yamadaoka, Suita, 565-0871, Japan
Nobuhiro Tsuji
Affiliation:
[email protected], Osaka University, Adaptive Machine Systems, 2-1, Yamadaoka, Suita, 565-0871, Japan
Get access

Abstract

We studied antiphase domain (APD) growth and lamellar structure formation during isothermal annealing of Ti-39at%Al single crystals at α2+γ dual phase temperature after quenching from α single phase state, intending to obtain a APD/lamellae mixed microstructure and to examine whether such a microstructure provides a strength higher than that obtained only by refining lamellar structure. The effect of plastic deformation prior to the annealing was also examined expecting a acceleration of γ lamellae formation through a preferential nucleation of γ-plates at dislocations. The lower was the annealing temperature, the smaller both the APD size and the lamellar spacing at the moment of a homogeneous lamellar structure formation tended to be, although naturally both the APD growth and the γ lamellae formation were slower. However, the APD size in the homogeneous lamellar structure was no smaller than 400 nm. A structure with finer APDs and finer lamellar structure was obtained by deforming the crystal before annealing since the lamellar structure formation was accelerated and the time for APD growth before the lamellar structure formation was shortened. For instance, a structure with an average lamellar spacing of 88 nm and an average APD size of 214 nm was obtained by deforming the crystals to 10 % plastic strain and subsequently annealing at 1073 K for 1×104 s, while no γ plate was obtained only by such an annealing without deformation.

Type
Research Article
Copyright
Copyright © Materials Research Society 2007

Access options

Get access to the full version of this content by using one of the access options below. (Log in options will check for institutional or personal access. Content may require purchase if you do not have access.)