Hostname: page-component-cd9895bd7-dzt6s Total loading time: 0 Render date: 2024-12-27T01:36:48.715Z Has data issue: false hasContentIssue false

Electrical Switching Using Compliant Metal Infiltrated Multi-Wall Nanotube Arrays

Published online by Cambridge University Press:  01 February 2011

Justin Bult
Affiliation:
[email protected], Rensselaer Polytechnic Institute, Materials Science and Engineering, 140 Materials Research Center, 110 8th St, Troy, NY, 12180, United States
W. Gregory Sawyer
Affiliation:
[email protected], University of Florida, Mechanical and Aerospace Engineering, Gainesville, FL, 32611, United States
Andrey Voevodin
Affiliation:
[email protected], Air Force Research Laboratory, Wright-Patterson AFB, OH, 45433, United States
Chris Muratore
Affiliation:
[email protected], Air Force Research Laboratory, Wright-Patterson AFB, OH, 45433, United States
Pam Dickrell
Affiliation:
[email protected], University of Florida, Mechanical and Aerospace Engineering, Gainesville, FL, 32611, United States
Sunil Pal
Affiliation:
[email protected], Rensselaer Polytechnic Institute, Materials Science and Engineering, Troy, NY, 12180, United States
Pulickel Ajayan
Affiliation:
[email protected], Rensselaer Polytechnic Institute, Materials Science and Engineering, Troy, NY, 12180, United States
Linda Schadler
Affiliation:
[email protected], Rensselaer Polytechnic Institute, Materials Science and Engineering, Troy, NY, 12180, United States
Get access

Abstract

The topology of conventional noble-metal-coated switch counterfaces creates modes of switch failure via fouling, arcing, and local melting when impacted. To avoid these failure phenomena, compliant conductive contact surfaces of vertically aligned multi-wall nanotube arrays grown on conductive substrates have been fabricated. Infiltration of the array by noble metal results in a robust compliant switch contact surface. Cyclic hot-switch testing of the nanotube based switch, via modified nano-indentation, results in performance surpassing conventional designs with stable resistance of 0.4Ω over 3000 cycles. Investigating the physical performance of the array shows the array is compacted less than 3% over the first 500 cycles with no observable compaction through the remaining cycles. The improvement in performance of the nanotube based switch is attributed to the ability for the compliant contact surface to conform to the probe tip geometry, increasing the effective contact surface area.

Type
Research Article
Copyright
Copyright © Materials Research Society 2008

Access options

Get access to the full version of this content by using one of the access options below. (Log in options will check for institutional or personal access. Content may require purchase if you do not have access.)

References

REFERENCES

1. Hyman, D. and Mehregany, M., IEEE Transactions on Components and Packaging Technology 22, 357 (1999)Google Scholar
2. Tringe, J.W., Uhlman, T.A., Oliver, A.C. and Houston, J.E., J. App. Phys. 93, 4661 (2003)Google Scholar
3. Tringe, J.W., Wilson, W. and Houston, J., “Reliability, Testing, and Characterization of MEMS/MOEMS,” ed. Ramesham, R. (Proc. SPIE, 2001) 4558 pp. 151158.Google Scholar
4. Greenwood, J.A. and Williamson, J.P., Proc. Royal Soc. (London) A295, 300 (1966).Google Scholar
5. Cao, A., Dickrell, P., Sawyer, W.G., Ghasemi-Nehjad, M. and Ajayan, P.M., Science 310, 1307 (2005).Google Scholar
6. Talapatra, S., Kar, S., Pal, S., Vajtai, R., Ci, L., Victor, P., Shaijumon, M., Kaur, S., Nalamasu, O., Ajayan, P., Nature Nanotechnology 1, 112 (2006).Google Scholar
7. Li, W., Xie, S., Qian, L., Chang, B., Zou, B., Zhou, W., Zhao, R., Wang, G., Science 274, 1701 (1996).Google Scholar
8. Hannoe, S. and Hosaka, H., Microsystem Technologies 3, 31 (1996).Google Scholar