No CrossRef data available.
Article contents
Elastic and Plastic Properties of Gamma + Laves Phase In-situ Composite Alloys Using Nanoindentation Techniques
Published online by Cambridge University Press: 10 February 2011
Abstract
In the present study, the local elastic and plastic properties of the γ- TiAl and the Laves phases have been investigated in a series of γ + Laves alloys using room-temperature compression, Vickers microhardness, and nanoindentation with an emphasis on elucidating the local property changes in γ + Laves alloys deformed at room temperature. This study shows that nanoindentation can be used to provide useful information on plastic flow in multiphase intermetallic alloys.
- Type
- Research Article
- Information
- Copyright
- Copyright © Materials Research Society 1999
References
REFERENCES
1.
Kim, Y. W. and Froes, F. H., High Temperature Aluminides and Intermetallics, ed. Whang, S. H., Liu, C. T., Pope, D. P. and Stiegler, J. O. (Warrendale, PA: The Minerals, Metals and Materials Society, 1989), 465–492.Google Scholar
2.
Yamaguchi, M., Titanium ‘92, ed. Froes, F. H. and Caplan, I. (Warrendale, PA: The Minerals, Metals and Materials Society, 1993), 959–970.Google Scholar
3.
Brady, M. P., Brindley, W. J., Smialek, J. L. and Locci, I. E., JOM, 8 (1996), 46–50.CrossRefGoogle Scholar
4.
McCarron, R. L., Schaeffer, J. C., Meier, G. H., Berztiss, D., Perkins, R. A. and Cullinan, J., Titanium ‘92, ed. Froes, F. H. and Caplan, I. (Warrendale, PA: The Minerals, Metals and Materials Society, 1993), 1971–1978.Google Scholar
5. Brady, M. P., Smialek, J. L. and Terepka, F., Scripta Metallurgica et Materialia, 32 (1995), 1659–1664.CrossRefGoogle Scholar
6. Perkins, R. A. and Meier, G. H., Proceedings of the Industry-University Advanced Materials Conference II, ed. F. Smith (Golden, CO: Advanced Materials Institute, 1989), 92.Google Scholar
7.
Tang, Z. L., Wang, F. H. and Wu, W. T., Oxidation of Metals, 48 (1997), 511–525.CrossRefGoogle Scholar
8.
Leyens, C., M., S., Peters, M. and Kaysser, W. A., Materials Science and Engineering A, A239–240 (1997), 680–687.CrossRefGoogle Scholar
9.
Brady, M. P., Smialek, J. L. and Brindley, W. J., US Patent 5,837,387 (November 17, 1998).Google Scholar
10.
Krushchov, M. M. and Berkovich, E. S., Industrial Diamond Review, 11 (1951), 42–49.Google Scholar
11.
Oliver, W. C. and Pharr, G. M., Journal of Materials Research, 7 (1992), 1564–1583.CrossRefGoogle Scholar
12.
Pethica, J. B. and Oliver, W. C., Thin Films: Stress and Mechanical Properties, ed. Bravman, J. C., Nix, W. D., Barnett, D. M. and Smith, D. A. (Pittsburgh, PA: Materials Research Society, 1989), 87–92.Google Scholar