The Effects of N2 and Ar as the Ambient Gas During Rapid Thermal Annealing of Tungsten Silicide
Published online by Cambridge University Press: 26 February 2011
Abstract
Rapid thermal annealing of amorphous tungsten silicide thin films (W0.62 Si0 38) on Si at 1100°C in Ar and N2 ambient gases was studied. All films annealed in N2 exhibited good adhesion and remained smooth with no large grain growth. Films annealed in Ar showed grain nucleation and growth from the film perimeter until a critical stress was achieved, followed by stress-assisted grain growth. The resulting growth of large columnar grains caused the films to delaminate. Removal of the surface oxide/nitride layer from the silicide prior to annealing resulted in uniform nucleation and growth over the entire film during annealing in Ar, with no stress-assisted grain growth or film delamination. No difference, however, was observed during annealing in N2. These results suggest that a surface film produced during annealing in N2 slows the nucleation and growth and consequently enhances film adhesion.
- Type
- Research Article
- Information
- Copyright
- Copyright © Materials Research Society 1988
References
1 Chen, John Y. and Roth, Lynette B., Solid State Technology 27 (8), 145, (1984).Google Scholar
2 Mohammadi, F. and Saraswat, K.C., J. Electrachem. Soc. 127 (2), 450 (1980).CrossRefGoogle Scholar
3 Shaw, J.M. and Amick, J.A., RCA Review 31 (2), 306 (1970).Google Scholar
4 Zirinsky, S., Hammer, W., d'Heurle, F., and Baglin, J., Appl. Phys. Lett. 33 (1), 76 (1978).CrossRefGoogle Scholar
5 Silversmith, D.J., Rathman, D.D., and Mountain, R.W., Thin Solid Films 93, 413 (1982).CrossRefGoogle Scholar
6 Bomchil, G., Goeltz, G., and Tortes, J., Thin Solid Films 140, 59 (1986).CrossRefGoogle Scholar
7 Chang, Chuan C. and Quintana, G., Journal of Electron Spectroscopy and Relatul Phenomena 2, 363, (1973).CrossRefGoogle Scholar
8 Nicolet, Marc-A., and Lau, S.S., in VLSI Electronics: Microstructure Science, Vol.6, edited by Einspruch, Norman G. and Larrabee, Graydon B. (Academic Press, New York, 1983) p. 409.Google Scholar
9 Siegal, M. (private communication).Google Scholar
10 Tsaur, B-Y., Chen, C.K., Anderson, C.H. Jr., and Kwong, D.L., J. Appl. Phys. 57 (6), 1890 (1985).CrossRefGoogle Scholar
11 Göltz, G., Torres, J., Lajzerowicz, J. Jr., and Bomchil, G., Thin Solid Films 124, 19 (1985).CrossRefGoogle Scholar
12 Tsai, M.Y., d'Heurle, F.M., Petersson, C.S., and Johnson, R.W., J. AppI. Phys. 52 (8), 5350 (1981).CrossRefGoogle Scholar
13 Sedgwick, T.O., d'Heurle, F.M., and Cohen, S.A., J. Electrachem. Sac. 131 (10), 2446 (1984).CrossRefGoogle Scholar
14 Choi, K.W. and Ahn, K. Y., J. Vac. Sci. and Technol. A 3 (6), 2272 (1985).CrossRefGoogle Scholar
15 Fukumoto, Masanori and Ohzone, Takashi, Appl. Phys. Lett. 50 (14), 894 (1987).CrossRefGoogle Scholar
16 Thomas, R.E. (private communication).Google Scholar
17 Thomas, R.E., Appl. Surface Sci. 26 534 (1986).CrossRefGoogle Scholar
- 2
- Cited by