Hostname: page-component-78c5997874-ndw9j Total loading time: 0 Render date: 2024-11-17T15:12:44.376Z Has data issue: false hasContentIssue false

Effects of Microadditions of Cerium on Annealing Embrittlement in FeBSi Glasses

Published online by Cambridge University Press:  26 February 2011

D. M. Kroeger
Affiliation:
Metals and Ceramics Division, Oak Ridge National Laboratory, Oak Ridge, TN 37831–6116
C. G. Mckamey
Affiliation:
Metals and Ceramics Division, Oak Ridge National Laboratory, Oak Ridge, TN 37831–6116
J. O. Scarbrough
Affiliation:
Metals and Ceramics Division, Oak Ridge National Laboratory, Oak Ridge, TN 37831–6116
Get access

Abstract

Microadditions of cerium retard annealing embrittlement in some but not all metallic glass compositions in the FeBSi system. Effects on embrittlement of doping with both cerium and oxygen have been determined for a series of compositions, FexB13 Si87-x. For X > 80, cerium retards annealing embrittlement and oxygen promotes it, suggesting that the beneficial effect of cerium additions results from gettering of impurities. The results indicate that for those compositions in the FeBSi system with the highest values of the saturation magnetization, Ms, microadditions of cerium can prevent annealing embrittlement until the onset of crystallization.

Type
Articles
Copyright
Copyright © Materials Research Society 1987

Access options

Get access to the full version of this content by using one of the access options below. (Log in options will check for institutional or personal access. Content may require purchase if you do not have access.)

References

1. Kroeger, D. M., Koch, C. C., McKamey, C. G., Scarbrough, J. O. and R. A. Padgett, RQM 5, Wurzburg, FRG, August 1984, 1369.Google Scholar
2. Kroeger, D. M., Canright, G. S., McKamey, C. G., Easton, D. S. and Scarbrough, J. O., Acta Met., to be published.Google Scholar
3. Canright, G. S. and Kroeger, D. M., IEEE Trans. Magnetics, MAG–22, 182 (1986).Google Scholar
4. Canright, G. S. and Kroeger, D. M., Mat. Res. Soc. Symp. Proc. Vol.58, 159 (1986).Google Scholar
5. Luborsky, F. E., Becker, J. J., Walter, J. L. and Liebermann, H. H., IEEE Trans. Magnetics, MAG–15, 1146 (1979).Google Scholar
6. DeCristofaro, N., Freilich, A. and Fish, G., J. Materials Science 17, 2365 (1982).Google Scholar
7. Spaepen, F. and Taub, A. I., “Amorphous Metallic Alloys,” ed. By Luborsky, F. E., Butterworths, London, 231 (1983).Google Scholar
8. Chen, H. S., Reports on Progress in Physics, 43, 353 (1980).Google Scholar
9. Piller, J. and Haasen, P., Acta Met. 30, 1 (1982).Google Scholar
10. Janot, C., George, B., Teirlinck, D., Marchal, G., Tete, C. and Delcroix, P., Phil. Mag, A 47, 301 (1983).Google Scholar
11. Spaepen, F., Tsao, S. S. and Wu, T. W., “Amorphous Metals and Semiconductors,” ed. by Haasen, P. and Jafee, R. I., Pergamon Press, Oxford, 365 (1986).Google Scholar
12. Kroeger, D.M. and Scarbrough, J. O., to be published.Google Scholar
13. Liebermann, H. H. and Luborsky, F. E., Acta Met. 29, 1413 (1981).Google Scholar