Hostname: page-component-586b7cd67f-2plfb Total loading time: 0 Render date: 2024-11-29T07:47:20.722Z Has data issue: false hasContentIssue false

Edge Effects of Nitride Film Patterning on Dislocation Generation in Local Oxidation of Silicon

Published online by Cambridge University Press:  10 February 2011

I. V. Peidous
Affiliation:
R&D Department, Chartered Semiconductor Mfg., Singapore 738406, [email protected]
R. Sundaresan
Affiliation:
R&D Department, Chartered Semiconductor Mfg., Singapore 738406
E. Quek
Affiliation:
R&D Department, Chartered Semiconductor Mfg., Singapore 738406
C. K. Lau
Affiliation:
R&D Department, Chartered Semiconductor Mfg., Singapore 738406
Get access

Abstract

Extensive monitoring of device characteristics in the manufacturing of ULSI with advanced LOCOS isolation revealed the strong dependence of device leakage currents on the process of patterning of silicon nitride films applied as a hard mask for local oxidation of silicon wafers. At the same time, the level of the leakage currents strongly correlated to stress-induced dislocation density in the device structures. Formation of microtrenches on the wafer surface at the nitride film edges was identified to have a major impact on the leakage currents. Surprisingly, structures having nitride film edge profiles with feet were consistently dislocation-free after the local oxidation. This showed that nitride etching process created surface damage that provided effective sites for crystal defect nucleation in silicon at the film edges. Computer simulations demonstrated that the feet at nitride edges substantially suppress stress growth during local oxidation.

Type
Research Article
Copyright
Copyright © Materials Research Society 1998

Access options

Get access to the full version of this content by using one of the access options below. (Log in options will check for institutional or personal access. Content may require purchase if you do not have access.)

References

1. Kenkare, P. U., Pfiester, J. R., Semiconductor International, 17 (5), 6468 (1994).Google Scholar
2. Chatterjee, A., Rojers, D., McKee, J., Ali, I., Nag, S., Chen, I. C. in IEDM Tech. Dig., 1996, pp. 829832.Google Scholar
3. Tanabe, Y., Suzuki, N., Natsuaki, N. in 4th Int. Conf on Advanced Thermal Processing of Semiconductors, RTP'96, Fair, R. B., Green, M. L., Lojek, B., Thakur, R.P.S., Eds., 1996, pp. 59.Google Scholar
4. Shibata, K., Taniguchi, K., J. Electrochem. Soc., 127 (6), 13831386 (1980).Google Scholar
5. Strunk, H. in Microsc. Semicond. Mater. Conf., Oxford, 2123 March 1983, Inst. Phys. Conf. Ser. No. 67: Section 10, 1983, pp. 451-459.Google Scholar
6. Smeys, P., Griffin, P. B., Rek, Z. U., Wolf, I. D., Saraswat, K. C. in IEDM Tech. Dig., 1996, pp. 709713.Google Scholar