Abstract

Diopside was prepared sintering a powder compact of composition CaMgSi2O6 at 1573K for 2 hours. The bending strength of this sintered body was 300MPa and fracture toughness was 3.5MPam1/2. Diopside was soaked in a simulated body fluid at 309.5K. Three days later diopside formed hydroxyapatite (Hap) all over the surface [1]. Diopside implanted in rabbits came in close contact with the newly grown bone. EPMA spectral diagrams show a change of composition across the junction from the diopside to the newly grown bone [2].

Type
Research Article
Copyright
Copyright © Materials Research Society 1992

Access options

Get access to the full version of this content by using one of the access options below. (Log in options will check for institutional or personal access. Content may require purchase if you do not have access.)

References

REFERENCES

1. Nakajima, S., The Shikwa Gakuho 89 (11) 1989.CrossRefGoogle Scholar
2. Nakajima, S., The Shikwa Gakuho 90 (4) 1990.CrossRefGoogle Scholar
3. Nonami, T., MRS Symposium proceedings 175 1989.CrossRefGoogle Scholar