A-Si:H Deposited by Direct Photo-Cvd Using a Microwave-Excited Xe Lamp

Published online by Cambridge University Press:  25 February 2011

Hiroyuki Matsunami
Affiliation:
Dept. of Electrical Engineering, Kyoto University, Sakyo, Kyoto, 606, Japan
Tatsuru Shirafuji
Affiliation:
Dept. of Electrical Engineering, Kyoto University, Sakyo, Kyoto, 606, Japan
Takashi Fuyuki
Affiliation:
Dept. of Electrical Engineering, Kyoto University, Sakyo, Kyoto, 606, Japan
Masahiro Yoshimoto
Affiliation:
Dept. of Electrical Engineering, Kyoto University, Sakyo, Kyoto, 606, Japan
Get access

Abstract

A-Si:H films were deposited by direct decomposition of Si2H6 using vacuum ultra-violet light (147nm) emitted from a microwave-excited Xe resonance lamp. The substrate temperature was varied between 200 and 300 °C . The hydrogen content in the films is estimated to be comparable or lower than that in high-quality glow discharge (GD) films based on results from infrared absorption measurements and hydrogen effusion measurements. Hydrogen atoms are incorporated in the form of Si-H bonds (2000 cm−1 mode), and Si-Hn bonds of the 2090 mode In a unit volume was one or two order less than that of Si-H bonds (2000 cm−1 mode). In spite of the lower hydrogen content, the defect density was lower than that of GD films. The mobility gap of the photo-CVD film was closer to the optical gap. For both n- and p-type doping, the dark conductivity increased with the dopant gas composition monotonously, and reached the order of 10−3 S/cm.

Type
Research Article
Copyright
Copyright © Materials Research Society 1990

Access options

Get access to the full version of this content by using one of the access options below. (Log in options will check for institutional or personal access. Content may require purchase if you do not have access.)

References

REFERENCES

Mishima, Y., Hirose, M. and Osaka, Y., J. Appl. Phys. 56, 2803 (1984).Google Scholar
[2] Fuyuki, T., Du, K., Okamoto, S., Yasuda, S., Kimoto, T., Yoshimoto, M. and Matsunami, H., J. Appl. Phys. 64, 2380 (1988).Google Scholar
[3] Perkins, G.G. and Lampe, F.W., J. Am. Chem. Soc. 102, 376 (1980).Google Scholar
[4] Ito, U., Toyoshima, Y. and Onuki, H., Washida, N. and Ibuki, T., J. Chem. Phys. 85 (1986) 4867.Google Scholar
[5] Shepard, K., Smith, Z.E., Aljishi, S. and Wagner, S., in Amorphous Silicon Technology, edited by Madan, A., Thompson, M.J., Taylor, P.C., LeComber, P.G. and Hamakawa, Y. (Mater. Res. Soc. Proc. 118, Pittsburgh, PA 1988) p.147.Google Scholar
[6] Madan, A., Muhl, S. and von Roedern, B., ibd., p.587.Google Scholar
[7] Cardona, M., Phys. Stat. Sol. b 118, 463 (1983).Google Scholar
[8] Curtins, H., Favre, M., Ziegler, Y., Wyrsch, N., Brechet, M. and Shah, A.V., in Amorphous Silicon Technology, edited by Madan, A., Thompson, M.J., Taylor, P.C., LeComber, P.G. and Hamakawa, Y. (Mater. Res. Soc. Proc. 118, Pittsburgh, PA 1988) p.159.Google Scholar
[9] Parsons, G., Tsu, D. and Lucovsky, G., Proc. 12th Int. Conf. Amorphous & Liquid Semiconductor, Prague, 1987, p.1375.Google Scholar
[10] Roca i Cabarrocas, P., Liu, J.Z., Park, H.R., Maruyama, A. and Wagner, S., Proc. 13th Int. Conf. Amorphous & Liquid Semiconductors, Nashville, USA, 1989, p.190.Google Scholar
[11] Vanecek, M., Kocka, J., Stuchlik, J., Koisek, Z., Stika, O. and Triska, A., Solar Energy Materials 8 (1983) 411.Google Scholar
[12] Wronski, C.R., Abels, B., Cody, G.D. and Cody, G.D., Solid State Communi. 44 (1982) 1423.Google Scholar
[13] Shimizu, T., Kido, H., Morimoto, A. and Kumeda, M., J. Appl. Phys. 28 (1989) 586.Google Scholar
[14] Wronski, C.R., Lee, S., Hicks, M. and Kumar, S., Phys. Rev. Lett. 63 (1989) 1420.Google Scholar