Alumina-Silicate Glass Interfacial Properties Probed by Micromechanical Testing Techniques

Published online by Cambridge University Press:  15 February 2011

Andrey V. Zagrebelnya
Affiliation:
Department of Chemical Engineering and Materials Science, University of Minnesota, 421 Washington Ave. SE., Minneapolis, MN 55455
John C. Nelson
Affiliation:
Department of Chemical Engineering and Materials Science, University of Minnesota, 421 Washington Ave. SE., Minneapolis, MN 55455
Erica T. Lilleodden
Affiliation:
Department of Chemical Engineering and Materials Science, University of Minnesota, 421 Washington Ave. SE., Minneapolis, MN 55455
Sundar Ramamurthy
Affiliation:
Department of Chemical Engineering and Materials Science, University of Minnesota, 421 Washington Ave. SE., Minneapolis, MN 55455
C. Barry Carter
Affiliation:
Department of Chemical Engineering and Materials Science, University of Minnesota, 421 Washington Ave. SE., Minneapolis, MN 55455
Get access

Abstract

Micromechanical properties of the interfaces between alumina and calcium-aluminosilicate (CAS) glasses were tested using various micro/nanoindentation techniques. The interfaces were produced by depositing continuous films of anorhtite (CaAl2Si2O8) onto single-crstal α-Al2O3 of two crystallographic orientations by pulsed-laser deposition (PLD).

The mechanical behavior of the interfaces was examined using two different depthsensing indentation instruments. Three types of tests, namely indentation, microscratch, and in-situ indentation combined with atomic force microscopy (AFM) imaging were conducted using different operating modes. The deformation behavior observed for the indentations and microscratches has been correlated with irregularities observed in the load-displacement curves. In the first two cases, scanning electron microscopy (SEM) has been used to characterize the deformation structures associated with the deformed regions. The in-situ experiments allow force-displacement measurements and AFM imaging immediately before and after indentation. The preindent and postindent morphology of the surface could then be characterized.

Type
Research Article
Copyright
Copyright © Materials Research Society 1996

Access options

Get access to the full version of this content by using one of the access options below. (Log in options will check for institutional or personal access. Content may require purchase if you do not have access.)

References

1. Clarke, D. R. and Gee, M. L., in Materials Interfaces: Atomic-level structure and properties, Wolf, D. and Yip, S. (ed.), Chapman & Hall, London (1992), p. 255.Google Scholar
2. Travitzky, N. A., Brandon, D. G. and Gutmanas, E. Y., Mater. Sci. Eng., 71, 65 (1985).Google Scholar
3. Mallamaci, M.P., Ph.D. Thesis, Cornell University 1995.Google Scholar
4. Ramamurthy, S., Mallamaci, M. P., Carter, C. B., Duncombe, P. R. and Shaw, T. M., 51st Annual Meeting MSA, Cincinnati, OH (1993), p. 948.Google Scholar
5. Susnitzky, D. W. and Carter, C. B., J. Am. Ceram. Soc., 69, C-217(1986).Google Scholar
6. Kotula, P. G. and Carter, C. B., Mater. Res. Soc. Symp. Proc., (1993), p. 373.Google Scholar
7. Wu, T. W., J. of Mat. Res., 6, 407, (1991).Google Scholar
8. Lilleodden, E. T., Bonin, W., Nelson, J., Wyrobek, J. T., and Gerberich, W. W., J. of Mat. Res., 10, 2162 (1995).Google Scholar