Thermoelectric properties of synthesized Mg2Si0.95-xGe0.05Sbx by spark plasma sintering

Published online by Cambridge University Press:  16 March 2015

Asumi Sasaki
Affiliation:
Department of Materials Science and Technology, Tokyo University of Science, 6-3-1 Niijyuku, Katsushika-ku, Tokyo 125-8585, Japan
Koya Arai
Affiliation:
Department of Materials Science and Technology, Tokyo University of Science, 6-3-1 Niijyuku, Katsushika-ku, Tokyo 125-8585, Japan
Yuto Kimori
Affiliation:
Department of Materials Science and Technology, Tokyo University of Science, 6-3-1 Niijyuku, Katsushika-ku, Tokyo 125-8585, Japan
Tomoyuki Nakamura
Affiliation:
Department of Materials Science and Technology, Tokyo University of Science, 6-3-1 Niijyuku, Katsushika-ku, Tokyo 125-8585, Japan SWCC Showa Cable Systems Co., Ltd., LTD, 4-1-1 Minami-Hashimoto Chuo-Ku Sagamihara, Kanagawa, Japan
Kenjiro Fujimoto
Affiliation:
Department of Pure and Applied Chemistry, Tokyo University of Science, 2641 Yamazaki, Noda-shi, Chiba 278-8510, Japan
Yuki Yamaguchi
Affiliation:
Department of Pure and Applied Chemistry, Tokyo University of Science, 2641 Yamazaki, Noda-shi, Chiba 278-8510, Japan
Ryuji Tamura
Affiliation:
Department of Materials Science and Technology, Tokyo University of Science, 6-3-1 Niijyuku, Katsushika-ku, Tokyo 125-8585, Japan
Tsutomu Iida
Affiliation:
Department of Materials Science and Technology, Tokyo University of Science, 6-3-1 Niijyuku, Katsushika-ku, Tokyo 125-8585, Japan
Keishi Nishio
Affiliation:
Department of Materials Science and Technology, Tokyo University of Science, 6-3-1 Niijyuku, Katsushika-ku, Tokyo 125-8585, Japan
Get access

Abstract

Magnesium silicide (Mg2Si) has attracted much interest as an n-type thermoelectric material because it is eco-friendly, non-toxic, light, and relatively abundant compared with other thermoelectric materials. In this study, we tried to improve the thermoelectric performance by doping Sb and Ge in the Mg2Si, as well as further optimizing x in the carrier concentration to cause phonon scattering. A high purity Mg2Si was synthesized from metal Mg and Sb doped Si-Ge alloy by using spark plasma sintering (SPS) equipment. The sintered samples were cut and polished. They were evaluated by using X-ray diffraction (XRD) and X-ray fluorescence (XRF) analyses. The carrier concentration of the samples was measured by using Hall measurement equipment. The electrical conductivity and Seebeck coefficient were measured by using a standard four-probe method in a He atmosphere. The thermal conductivity was measured by using a laser-flash system. We succeeded in obtaining a Sb doped Mg2Si0.95Ge0.05 sintered body easily without any impurities with the SPS equipment. The electrical conductivity of the sample was increased, and thermal conductivity was decreased by increasing the amount of doped Sb. The dimensionless figure of merit ZT became 0.74 at 733 K in the Mg2Si0.95-xGe0.05Sbx sample with x = 0.0022.

Type
Articles
Copyright
Copyright © Materials Research Society 2015 

Access options

Get access to the full version of this content by using one of the access options below. (Log in options will check for institutional or personal access. Content may require purchase if you do not have access.)

References

Heller, M. W. and Danielson, G. C., J. Phys. Chem. Solids 23, 601 (1962)CrossRefGoogle Scholar
LaBotz, R. J., Mason, D. R., and O’Kane, D. F., J. Electrochem. Soc. 110, 121 (1963)CrossRefGoogle Scholar
Noda, Y., Kon, H., Furukawa, Y., Otsuka, N., Nishida, I., and Matsumoto, K., Mater. Trans. JIM 33, 845 (1992)CrossRefGoogle Scholar
Tani, J. and Kido, H., Physica B 223, 364 (2005)Google Scholar
Zaitsev, V. K., Fedorv, M. I., Gurieva, E. A., Eremin, I. S., Konstantinov, P. P., Samunin, A. Yu., and Vedernikov, M. V., Phys. Rev. B74, 045207 (2006)CrossRefGoogle Scholar
Akasaka, M., Iida, T., Nemoto, T., Soga, J., Soga, J., Sato, J., Makino, K., Fukano, M., and Takanashi, Y., J. Cryst. Growth 304, 196 (2007)CrossRefGoogle Scholar
Sakamoto, T., Iida, T., Kurosaki, S., Yano, K., Taguchi, H., Nishio, K., and Takanashi, Y., J. Electron. Mater. 40, 629 (2011)CrossRefGoogle Scholar
Zhou, X., Wang, G., Chi, H., J. Electron. Mater. 41, 6 (2012)Google Scholar
Garg, J., Bonini, N., Kozinsky, B. and Marzari, N., PHYSICAL REVIEW LETTERS, 106, 045901 (2011)CrossRefGoogle Scholar
Mori, Y., Kaihara, Y., Nakamura, S., Yoshio, T., and Takarabe, K., Phys. status solidi, 10, 12, 18471849 (2013)CrossRefGoogle Scholar
Dasgupta, T., et al. ., PHYSICAL REVIEW B 83, 235207 (2011)CrossRefGoogle Scholar
Nolas, G. S., et al. ., PHYSICAL REVIEW B 76, 235204 (2007)CrossRefGoogle Scholar
Kajikawa, T., Shida, K, Sugihara, S., Proc. ICT ’97, 14th International Conference on Thermoelectrics (1997)Google Scholar
Tani, J. and Kido, H., Intermetallics 15 (2007) 12021207 CrossRefGoogle Scholar
You, Sin-Wook, SHIN, Dong-Kil, KIM, Il-Ho, J.Korean Phys.Vol. 64, No9, May 2014, pp. 1346∼1350Google Scholar