Hostname: page-component-586b7cd67f-t7czq Total loading time: 0 Render date: 2024-11-23T13:18:42.847Z Has data issue: false hasContentIssue false

Superconducting characteristics of MgB2 wires obtained by Reactive Liquid Mg Infiltration

Published online by Cambridge University Press:  01 February 2011

Giovanni Giunchi
Affiliation:
[email protected], EDISON SpA, R&D, Foro Buonaparte 31, MILANO, N/A, 20121, Italy, +39-02-62223194, +39-02-62223074
Giovanni Ripamonti
Affiliation:
[email protected], EDISON SpA, MIlano, N/A, 20121, Italy
Elena Perini
Affiliation:
[email protected], EDISON SpA, MIlano, N/A, 20121, Italy
Tommaso Cavallin
Affiliation:
[email protected], CNR-IENI - Sezione di Lecco, Lecco, N/A, 23900, Italy
Enrico Bassani
Affiliation:
[email protected], CNR-IENI - Sezione di Lecco, Lecco, N/A, 23900, Italy
Umberto Gambardella
Affiliation:
[email protected], CNR-INFM SUPERMAT Lab., University ofSalerno, Baronissi, SA, 84081, Italy
Yifeng Yang
Affiliation:
[email protected], University of Southampton, Institute of Cryogenics, Southampton, N/A, SO17 1BJ, United Kingdom
Edward A. Young
Affiliation:
[email protected], University of Southampton, Institute of Cryogenics, Southampton, N/A, SO17 1BJ, United Kingdom
Marco Bianchetti
Affiliation:
[email protected], University of Southampton, Institute of Cryogenics, Southampton, N/A, SO17 1BJ, United Kingdom
Carlo Beduz
Affiliation:
[email protected], University of Southampton, Institute of Cryogenics, Southampton, N/A, SO17 1BJ, United Kingdom
Get access

Abstract

Superconducting MgB2 wires, of different diameter and length, have been produced by the reactive Liquid Mg Infiltration process, also implemented with the addition of extra Mg, to completely fill the internal hole created from the normal infiltration process. The actual wires have an Iron external lining and the metallic Mg internally added has a twofold effect: to avoid Mg deficiency during the reaction and to increase the quenching resistance of the wire. The superconducting characteristics of the wires have been measured either at the liquid He and at the liquid Ne temperatures, on small samples cut from meter long wires. The typical critical current density in self field, at 27.1 K, is about 1000 A/mm2, a value of interest for many power applications. The extension of the manufacturing process to longer wire will be discussed as well as the effect of the metallic lining of the wires on the contact resistance and on the current injection length.

Type
Research Article
Copyright
Copyright © Materials Research Society 2006

Access options

Get access to the full version of this content by using one of the access options below. (Log in options will check for institutional or personal access. Content may require purchase if you do not have access.)

References

1 Sumption, MD, Bhatia, M, Rindfleisch, M, Tomsic, M and , EWCollings, Supercond. Sci. Technol. 19, 155160 (2006).Google Scholar
2 Grasso, G, Malagoli, A, Ferdeghini, C, Roncallo, S, Braccini, V, Cimberle, MR and Siri, AS Appl.Phys. Lett. 79 230 (2001). R Musenich, P Fabbricatore, S Farinon, M Greco, M Modica, R Marabotto, R Penco, M Razeti and D Nardelli, Supercond. Sci. Technol. 19, S126–S131(2006).Google Scholar
3 Pachla, W, Morawski, A, Kovac, P, Husek, I, Mazur, A, Lada, T, Diduszko, R, Melisek, T, Strbik, V and Kulczyk, M,Supercond. Sci. Technol. 19, 18 (2006).Google Scholar
4 Serquis, A, Civale, L, Coulter, JY, Hammon, DL, Liao, XZ, Zhu, YT, Peterson, DE, Mueller, FM, Nesterenko, VF, and Indrakanti, SS, Supercond. Sci. Technol. 17, L35–L37 (2004).Google Scholar
5 Goldacker, W, Schlachter, SI, Obst, B, Eisterer, M Supercond Sci Technol. 17, S4905 (2004).Google Scholar
6 Tanaka, K, Kitaguchi, H, Kumakura, H, Hirakawa, M,Yamada, H and Okada, M IEEE Trans. Appl. Superconductivity 15, 31803183 (2005).Google Scholar
7 Togano, K, Nakane, T, Fujii, H, Takeya, H and Kumakura, H, Supercond Sci Technol.; 19 :L17–L20 (2006).Google Scholar
8 Flukiger, R, Suo, HL, Musolino, N, Beneduce, C, Toulemonde, P, Lezza, P, Physica C 385, 286305 (2003).Google Scholar
9 EDISON SpA Ital. Pat. Appl. MI2002A001004 (May 10,2002) US Patent N. 6,957,480 (Oct 25, 2005).Google Scholar
10 Giunchi, G Int. Journal of Modern Physics B Vol. 17, N. 4,5,6 453460 (Mar 2003)Google Scholar
11 Giunchi, G,Ceresara, S, Ripamonti, G, DiZenobio, A, Rossi, S, Chiarelli, S, Spadoni, M, Wesche, R, Bruzzone, PL, Supercond Sci Technol.; 16: 285291 (2003)Google Scholar
12 Giunchi, G, Orecchia, C, Malpezzi, L, Masciocchi, N PhysicaC 433, 182188 (2006)Google Scholar
13 Bharathi, A, Balaselvi, SJ, Kalavathi, S, Reddy, GLN,Sastry, VS, Hariharan, Y, Radhakrishnan, TS, Physica C 370 211 (2002).Google Scholar
14 Bianchetti, M, Al-Mosawi, M, Giunchi, G, Yang, Y, Beduz, C, Adv. in Cryo. Eng. Transaction of CEC, vol 51,729734 (2006)Google Scholar
15 Superconductor Week, vol 20, N 1, Jan 27, 2006 Google Scholar