Hostname: page-component-586b7cd67f-r5fsc Total loading time: 0 Render date: 2024-11-23T07:19:06.588Z Has data issue: false hasContentIssue false

Photochromic Organic-Inorganic Hybrid Nanocomposite Hard Coatings With Tailored Fast Switching Properties

Published online by Cambridge University Press:  10 February 2011

M. Mennig
Affiliation:
Institute for New Materials, GmbH, Im Stadtwald 43, D- 66123 Saarbruecken, Germany
K. Fries
Affiliation:
Institute for New Materials, GmbH, Im Stadtwald 43, D- 66123 Saarbruecken, Germany
H. Schmidt
Affiliation:
Institute for New Materials, GmbH, Im Stadtwald 43, D- 66123 Saarbruecken, Germany
Get access

Abstract

A recently developed photochromic organic-inorganic nanocomposite (Nanomer®) coating system is investigated, which is based on an epoxysilane as network former, different bisepoxides as spacer and an organic amine as thermal cross-linker. This coating system is compatible with different photochromic dyes like oxazines, pyrans and fulgides and also with surface modified ceramic nanoparticles as filler in order to obtain macroscopic “hard properties” without changing the photochromic kinetics. In order to investigate the dye-spacer interactions and influence on the switching kinetic behavior, the matrix composition was diminished to the network former, the thermal cross-linker and two types (polar and nonpolar) of spacers in different concentrations. Four commercially available spirooxazines with different molecular sizes and polarities were incorporated into the matrices and coatings on glass slides were prepared by float-coating and cured at 130 °C for 2 h. The half darkening and half fading times of the coatings were measured by a fast diode array spectrometer as a function of spacer type and concentration for the four different dyes. The “nonpolar” spacer CHMG did not influence the switching kinetic of the dyes significantly and fast switching times of 2 s - 4 s were obtained. The “polar” spacer PCF (aromatic character) showed interactions with the dye molecules, which led to an increase in the switching times of up to 25 s. The retardation of the switching process increased with increasing spacer content and with increasing polar character of the dye molecule. From these results, it could be concluded that the photochromic behavior of the spirooxazines could be adjusted to different applications by interactions with polar spacers.

Type
Research Article
Copyright
Copyright © Materials Research Society 1999

Access options

Get access to the full version of this content by using one of the access options below. (Log in options will check for institutional or personal access. Content may require purchase if you do not have access.)

References

REFERENCES

[1] Photochromism, Molecules and Systems, H., Dürr, H., Bouas-Laurent, eds., Elsevier, Amsterdam, Oxford, New York, Tokyo (1990)Google Scholar
[2] Crano, J.-P., Weber, S., Tardieu, P., Lelard, N., WO 96/27488 (1996)Google Scholar
[3] Hou, L., Hoffmann, B., Mennig, M., Schmidt, H., presented at the 17th International Congress on Glass, Oct 914 (1995), Beijing, China Google Scholar
[4] Schaudel, B., Guermeur, C., Sanchez, C., Nakatani, K. and Delaire, J. A., J. Mater. Chem. 7 (1), 61 (1997)10.1039/a606859fGoogle Scholar
[5] Sanchez, C., Proceeding of The Sixth International Symposium on New Glass, Oct. 14. - 15., 1997, Kikai - Shinko - Kaikan, p 1335 Google Scholar
[6] Levy, D. and Avnir, D., J. Phys. Chem. 92, 734 (1988)10.1021/j100327a035Google Scholar
[7] Levy, D., Einhorn, S. and Avnir, D., J. Non-Cryst. Solids 113, 137 (1989)10.1016/0022-3093(89)90004-5Google Scholar
[8] Preton, D., Pouxviel, J. C., Novinson, T., Kaska, W. C., Dunn, B. and Zink, J. I., J. Phys. Chem. 94, 4167 (1990)10.1021/j100373a054Google Scholar
[9] Nakazumi, H., Nagashiro, R., Matsumoto, S. and Isagawa, K., SPIE Proc. Vol. 2288, Sol-Gel Optics Ill, San Diego, 1994 Google Scholar
[10] Hou, L., Hoffmann, B., Mennig, M. and Schmidt, H., J. Sol-Gel Sci. Techn. 2, 635 (1994)10.1007/BF00486324Google Scholar
[11] Hou, L., Mennig, M. and Schmidt, H., Proc. Eurogel ”;92, 173 (1992)Google Scholar
[12] Biteau, J., Chaput, F. and Boilot, J. P., J. Phys. Chem. 100, 9024 (1996)10.1021/jp953607oGoogle Scholar
[13] Malatesta, V., Book Chapter 10 for ,,Photochromic and Thermochromic Compounds”;, Plenum Press, No.4, USA (1997)Google Scholar
[14] Hou, L., Hoffmann, B.-, Schmidt, H., Mennig, M., Sol-Gel Sci. Techn. 8, 923 (1997) and 927 (1997)Google Scholar
[15] Mennig, M., Fries, K. and Schmidt, H., Proc. 2nd Int. Conf. Coatings on Glass ICCG, SaarbrCicken 1998, accepted for publication in Thin Solid Films, 1999 Google Scholar
[16] Mennig, M., Fries, K. and Schmidt, H., Deutsche Glastechnische Berichte, 1999 (accepted for publication)Google Scholar
[17] catalogue information of Sigma-AldrichGoogle Scholar