Performance Characteristics of Low-Temperature Co Oxidation Catalysts

Published online by Cambridge University Press:  15 February 2011

Gar B. Hoflund
Affiliation:
Department of Chemical Engineering, University of Florida, Gainesville, FL 32611
Steven D. Gardner
Affiliation:
Department of Chemical Engineering, University of Florida, Gainesville, FL 32611
David R. Schryer
Affiliation:
NASA Langley Research Center, Hampton, VA 23665
Billy T. Upchurch
Affiliation:
NASA Langley Research Center, Hampton, VA 23665
Jacqueline Schryer
Affiliation:
NASA Langley Research Center, Hampton, VA 23665
Erik J. Kielin
Affiliation:
NASA Langley Research Center, Hampton, VA 23665
Get access

Abstract

A series of Au/MnOx catalysts with the Au content ranging from 0 to 10 at%, a 19.5 wt% Pt/SnOx catalyst and a commercially available 2 wt% Pt/SnOx catalyst have been examined for activity toward low-temperature CO oxidation. A 1 atm, 10 sccm stoichiometric mixture of CO (1 vol.%) and O2 in He were reacted at 55°C over 100 mg of each catalyst for time periods as long as 20,000 min. Under these conditions a 10 at% Au/MnOx catalyst exhibits the highest activity and the lowest decay. Outgassing experiments indicate that CO2 retention is primarily responsible for the activity decay of the Pt/SnOx catalysts and that the 10 at% Au/MnOx catalyst is not significantly affected by this process.

Type
Research Article
Copyright
Copyright © Materials Research Society 1995

Access options

Get access to the full version of this content by using one of the access options below. (Log in options will check for institutional or personal access. Content may require purchase if you do not have access.)

References

REFERENCES

1. Stark, D.S., Crocker, A. and Steward, G.J., J. Phys. E: Sci. Instrum. 16, 158 (1983).Google Scholar
2. Stark, D.S. and Harris, M.R., J. Phys. E: Sci. Instrum. 16,492 (1983).Google Scholar
3. Stark, D.S. and Harris, M.R., J. Phys. E: Sci. Instrum. 21, 715 (1988).Google Scholar
4. Batten, C.E., Miller, I.M., Wood, G.M. Jr., and Willetts, D.V., Eds., “Closed-Cycle, Frequency-Stable CO2 Laser Technology,” Proceedings of a workshop held at NASA Langley Research Center, Hampton, VA, June 1012, 1986, NASA Conference Publication 2456.Google Scholar
5. Schryer, D.R. and Hoflund, G.B., Eds., “Low-Temperature CO-Oxidation Catalysts for Long- Life C02 Lasers,” Collected papers from an international conference held at NASA Langley Research Center, Hampton, VA, October 1719, 1989, NASA Conference Publication 3076.Google Scholar
6. Gardner, S.D., Hoflund, G.B., Schryer, D.R., Schryer, J., Upchurch, B.T. and Kielin, E.J., Langmuir 7, 2135 (1991).Google Scholar
7. Haruta, M., Kobayashi, T. and Yamada, N., Chem. Lett. 405 (1987).Google Scholar
8. Haruta, M., Yamada, N., Kobayashi, T. and lijima, S., J. Catal. 115, 301 (1989).Google Scholar
9. Schryer, D.R., Upchurch, B.T., Norman, J.D. Van, Brown, K.G. and Schryer, J., J. Catal. 122, 193 (1990).Google Scholar
10. Schryer, D.R., Upchurch, B.T., Sidney, B.D., Brown, K.G., Hoflund, G.B. and Herz, R.K., J. Catal. 130, 314 (1991).Google Scholar
11. Gardner, S.D., Hoflund, G.B., Schryer, D.R. and Upchurch, B.T., J. Phys. Chem. 95, 835 (1991).Google Scholar
12. Drawdy, J.E., Hoflund, G.B., Gardner, S.D., Yngvadottir, E. and Schryer, D.R., Surface Inter. Anal. 16, 369 (1990).Google Scholar
13. “Catalysts for Long Range CO2 Laser System,” a progress report from a catalyst development program carried out by GEC Avionics, UK Atomic Energy Authority Harwell and UOP Ltd. under the auspices of the Royal Signals and Radar Establishment, November, 1988. Contract nl. SDIO 84-87-C-0046.Google Scholar