Abstract

XAS was used to investigate the oxidation behavior of Ni3Al aluminides with and without the addition of Cr. At 450 C the Cr formed a Cr2O3 like oxide layer which inhibited the oxidation of the Ni at the surface. Ni oxidation did occur in the sample without Cr at 450 C. At higher temperatures the Ni at the surface oxidized to NiO, but in the bulk no oxidation of the Ni was observed whether Cr was present or not. When no Cr was present a minimum was observed at 700 C in the fraction of oxidized Ni. The Cr (8at.%) did not cluster and substituted for Ni or Al in the Ni3Al aluminide.

Type
Research Article
Copyright
Copyright © Materials Research Society 1991

Access options

Get access to the full version of this content by using one of the access options below. (Log in options will check for institutional or personal access. Content may require purchase if you do not have access.)

References

REFERENCES

[1] Liu, C.T. and Sikka, V.K., J. Metals 38, 1921 (1986).Google Scholar
[2] Greegor, R.B., Lytle, F.W., Ewing, R.C. and Haaker, R.F., Nucl. Instr. and Meth. B1, 587 (1984).CrossRefGoogle Scholar
[3] Wyckoff, R.W.G., Crystal Structures, Vol. I & II (Interscience Publishers, New York, 1963).Google Scholar