Hostname: page-component-586b7cd67f-t8hqh Total loading time: 0 Render date: 2024-11-25T15:16:56.961Z Has data issue: false hasContentIssue false

Mechanism of the Suppression of Zr Silicide Formation in Poly-Si/ZrON/ZrSiON/Si Structure

Published online by Cambridge University Press:  01 February 2011

Masato Koyama
Affiliation:
Advanced LSI Technology Laboratory
Kyoichi Suguro
Affiliation:
3Process & Manufacturing Engineering Center, Semiconductor Company, Toshiba Corporation, 8 Shinsugita-cho, Isogo-ku, Yokohama 235-8522 Japan
Chie Hongo
Affiliation:
Environmental Engineering and Analysis Center
Mitsuo Koike
Affiliation:
Environmental Engineering and Analysis Center
Yuichi Kamimuta
Affiliation:
Environmental Engineering and Analysis Center
Masamichi Suzuki
Affiliation:
Environmental Engineering and Analysis Center
Akira Nishiyama
Affiliation:
Advanced LSI Technology Laboratory
Get access

Abstract

In this paper, the mechanisms of the suppression of Zr-silicide formation in poly-Si/ZrON/interfacial-layer/Si structure at 1000°C annealing are discussed in detail. It was demonstrated that gaseous SiO desorption, which played a dominant role in the silicide formation in the case of the ZrO2/SiO2/Si, was completely inhibited in the ZrON/interfacial-layer/Si structure. In addition, we have found that an ultrathin interfacial SiON layer between poly-Si and ZrON stabilized the interface. Consequently, we concluded that the effective nitrogen incorporation into top/bottom interfacial SiON layers with our process was responsible for the superior thermal stability of the stack.

Type
Research Article
Copyright
Copyright © Materials Research Society 2002

Access options

Get access to the full version of this content by using one of the access options below. (Log in options will check for institutional or personal access. Content may require purchase if you do not have access.)

References

[1] Lee, C.H. et al., Tech.Dig.IEDM 2000, p.27.Google Scholar
[2]Jeon, T.S.,White, J.M. and Kwong, D.L., Appl.Phys.Lett.,vol.78,2001, p.368.Google Scholar
[3]Kim, Y. et al., Tech.Dig.IEDM 2001, p.455.Google Scholar
[4]Hobbs, C. et al, Tech.Dig.IEDM 2001, p.651.Google Scholar
[5]Koyama, M., Suguro, K., Yoshiki, M., Kamimuta, Y., Koike, M., Ohse, M., Hongo, C. and Nishiyama, A., Tech.Dig.IEDM 2001, p.459.Google Scholar
[6]Maria, J.P., Wicaksana, D., Kingon, A.I., Busch, B., Schulte, H., Garfunkel, E. and Gustafsson, T., J.Appl.Phys.,vol.90,2001, p.3476.Google Scholar
[7]Muraoaka, K., (submitted to Apll.Phys.Lett.).Google Scholar
[8]Gutowski, M., Jaffe, J.E., Liu, C.-L., Stoker, M., Hegde, R.I., Rai, R.S. and Tobin, P.J., Appl.Phys.Lett., vol.80,2002, p.1897.Google Scholar