Hostname: page-component-586b7cd67f-2brh9 Total loading time: 0 Render date: 2024-11-25T17:36:22.575Z Has data issue: false hasContentIssue false

Laser Trim Revisited in the Light of an Excimer Lasera

Published online by Cambridge University Press:  25 February 2011

Michel Gauthier
Affiliation:
Laser Chemistry Group, Division of Chemistry, National Research Council of Canada, Ottawa, Canada, K1A 0R6
Richard Bourret
Affiliation:
NRC Summer Student 1988
Gerard Gavrel
Affiliation:
Network Access Division, Northern Telecom Canada Limited, P.O. Box 1000, Aylmer, Québec, Canada, J9H 5M6
Richard Carnegie
Affiliation:
Network Access Division, Northern Telecom Canada Limited, P.O. Box 1000, Aylmer, Québec, Canada, J9H 5M6
Get access

Abstract

In the Laser Chemistry Group's program aimed at understanding the basic mechanisms involved in the fabrication and characterization of integrated circuits, we have converted an infrared laser-based, thick film trimming technique, which is over 15 years old, to UV light. It is known that excimer lasers can be used for microfabrication of semiconductors and ceramics. Much cleaner ablations than those obtainable with the infrared lasers have been demonstrated in a large variety of materials. This, together with the fact that excimers with repetition rates over 1 kHz are presently on the market, leads us to propose that better accuracies and smaller drifts, should be achievable using excimer laser-based thick film hybrid circuit trimming. Results of XeCl laser trimming of over four hundred resistors, including temperature coefficient of resistance measurements and life tests at elevated temperatures, demonstrate that UV trimming is a factor of 10 better than the presently used infrared process.

Type
Research Article
Copyright
Copyright © Materials Research Society 1989

Access options

Get access to the full version of this content by using one of the access options below. (Log in options will check for institutional or personal access. Content may require purchase if you do not have access.)

Footnotes

a

Issued as NRCC # 29822

References

REFERENCES

1 Crawley, M.C., in Industrial Applications of Lasers, edited by Koebner, H. (Wiley, Chichester, 1984) pp. 177190.Google Scholar
2For the use of cermet pastes in the fabrication of thick film resistors, the reader is referred to textbooks such as: Harper, C.A., editor, Handbook of Thick Film Hybrid Microelectronics: A Practical Sourcebook for Designers. Fabricators. and Users, (McGraw-Hill, New York, 1974).Google Scholar
3Thin film circuits, formed by chemical etching of 0.1 μm thick coatings can also be laser trimmed. This is a different technology, not addressed in the present paper.Google Scholar
4The drift is the change in resistance with time, and is usually given in percent of the initial resistance value.Google Scholar
5 Schmatjko, K.J. and Endres, G., Fachber. Metallbearb. 64, 294 (1987).Google Scholar
6 Spalding, I.J., in Proc. 4th Int. Conf. Lasers in Manufacturing, edited by Steen, W.M. (IFS Ltd, Bedford, UK, 1987) pp. 229234.Google Scholar
7 Poulin, D., Reid, J., and Znotins, T., in Laser Materials Processing: Proc. 6th Int. Congress on Applications of Lasers and Electro-optics, edited by Ream, S.L., (IFS Publications, Bedford, UK, 1988) pp. 135141.Google Scholar
8 Jadin, A., Wautelet, M., and Laude, L.D., Semicond. Sci. Technol. 3, 499 (1988).Google Scholar
9 Sona, A., in Laser Advanced Materials Processing, (High Temperature Soc. Japan, Osaka, Japan, 1987) pp. 661673.Google Scholar
10 Humphries, M., Kahlert, H.-J., and Pippert, K., in Proc. 4th Int. Conf. Lasers in Manufacturing, edited by Steen, W.M. (IFS Ltd, Bedford, UK, 1987) pp. 255262.Google Scholar
11 Sandwell, R. (private communication).Google Scholar
12 Soni, P.R. and Rajan, T.V., Trans. Indian Ceramic Soc. 44, 42 (1985).Google Scholar
13 Wallace, R.L. and Copley, S.M., Adv. Ceramic Materials 1, 277 (1986).Google Scholar
14 Yamamoto, J. and Yamamoto, Y., in Laser Advance-d Materials Processing, (High Temperature Soc. Japan, Osaka, Japan, 1987) pp. 297302.Google Scholar
15 Miyamoto, I., Maruo, H., Kuriyama, K., and Horiguchi, Y., in Laser Advanced Materials 16 Processing, (High Temperature Soc. Japan, Osaka, Japan, 1987) pp. 237242.Google Scholar
16 Harrysson, R. and Herbertsson, H., in Proc. 4th Int. Conf. Lasers in Manufacturing, edited by Steen, W.M. (IFS Ltd, Bedford, UK, 1987) pp. 211220.Google Scholar
17 Cooper, K.P. and Ayers, J.D., in Laser Materials Processing: Proc. 6th Int. Congress on Applications of Lasers and Electro-optics, edited by Ream, S.L., (IFS Publications, Bedford, UK, 1988) pp. 179187.Google Scholar
18 Ito, S., Nakamura, M., and Kanematsu, W., Bull. Japan Soc. Precision Engg 21, 167 (1987).Google Scholar
19 Morita, N., Ishida, S., Fujimori, Y., and Ishikawa, K., Appl. Phys. Lett. 52, 1965 (1988).Google Scholar
20 Sturrett, M.S., in Proceedings of the 1987 International Symposium on Microelectronics, (Int. Soc. for Hybrid Microelectronics, Reston, VA 1987) pp. 140146.Google Scholar
21The Temperature Coefficient of Resistance, TCR, is the fractional change in resistance with temperature, and is usually given in parts per million, ppm, of the initial resistance value, per degree Celsius.Google Scholar