In Situ TEM Observation of Defects and Amorphous Phase in Si Wafer During Ion Implantation

Published online by Cambridge University Press:  28 February 2011

Naoto Shigenaka
Affiliation:
Energy Res. Lab., Hitachi Ltd., 1168 Moriyama, Hitachi, Ibaraki, 316, Japan
Tuneyuki Hashimoto
Affiliation:
Energy Res. Lab., Hitachi Ltd., 1168 Moriyama, Hitachi, Ibaraki, 316, Japan
Motomasa Fuse
Affiliation:
Energy Res. Lab., Hitachi Ltd., 1168 Moriyama, Hitachi, Ibaraki, 316, Japan
Nobuo Owada
Affiliation:
Device Development Center, Hitachi Ltd., 2326 Imai, Ome, Tokyo, 198, Japan
Hizuru Yamaguchi
Affiliation:
Device Development Center, Hitachi Ltd., 2326 Imai, Ome, Tokyo, 198, Japan
Seiko Ozono
Affiliation:
Device Development Center, Hitachi Ltd., 2326 Imai, Ome, Tokyo, 198, Japan
Get access

Abstract

In situ TEM observations of defects and. the amorphous phase in Si wafer during 150 keV Ar+ ion implantation were made which elucidated their characteristic behavior in Si. Defects introduced by ion implantation were eliminated by amorphous phase formation and then new defects did not form in the amorphous phase. Microstructural evolution in Si wafers under high dose implantation (2E16 ions/cm2) of 400 keV Si* ions was also investigated at temperatures of -70, -30, 20, 100 and 200 °C using a cross-section 1 TEM observation technique. At temperature of 20 °C and above, a defect layer was formed in each specimen, and the defect density was observed to decrease as temperature increased. At temperture of -30 °C and below the amorphous phase was formed and a defect layer which made contact with this phase was also observed. After annealing of these implanted specimens at 850 °C for 20 min, the amorphous phase had crystallized and the defect layer in contact with the amorphous phase was almost eliminated. But another defect layer was formed during annealing in the region where the amorphous phase had existed.

Type
Research Article
Copyright
Copyright © Materials Research Society 1992

Access options

Get access to the full version of this content by using one of the access options below. (Log in options will check for institutional or personal access. Content may require purchase if you do not have access.)

References

REFERENCES

[1] Tamura, M., Natsuaki, N., Wada, Y. and Mitani, E., J. Appl. Phys., 59 (1986) 3417 CrossRefGoogle Scholar
[2] Tamura, M. and Natsuaki, N., Jpn. J. Appl. Phys., 25 (1986) L474 CrossRefGoogle Scholar
[3] Tamura, M., Natsuaki, N., Wada, Y. and Mitani, E., Nucl. Instr. and Meth. B21 (1987) 438 CrossRefGoogle Scholar
[4] Tamura, M. and Suzuki, T., Nucl. Instr. and Meth. B39 (1989)Google Scholar
[5] Suzuki, K., Shigenaka, N., Nishimura, E. and Hashimoto, T., Nucl. Instr. and Meth. B24/25 (1987) 591 CrossRefGoogle Scholar
[6] Shigenaka, N., Nishimura, E., Hashimoto, T. and Suzuki, K., Nucl. Instr. and Meth. B51 (1990) 301 CrossRefGoogle Scholar
[7] Hashimoto, T., Proc. ASTM STP 1046 (1989) 523 Google Scholar
[8] Gibbons, J.F., Proc. IEEE, 60 (1972) 1062 CrossRefGoogle Scholar