Hydrogen-Enhanced SCC of 304 Austenitic Stainless Steel in MgCl2
Published online by Cambridge University Press: 10 February 2011
Abstract
SCC of 304 stainless steel(ss) in boiling MgCl2 at 416K was performed to investigated the effect of hydrogen during test. Results showed that the existence of hydrogen enhanced the susceptibility of SCC of 304ss. The fractography of specimen charged with hydrogen contained more intergranular than that of uncharged ones, and for the both specimens charged or uncharged with hydrogen, SCC initiated and propagated along { 111 } plane.
- Type
- Research Article
- Information
- Copyright
- Copyright © Materials Research Society 1998
References
REFERENCES
4.
Bastien, P., Azou, P., Proceedings frist world metal congress, ASM Metals Park, Ohio, 535(1951).Google Scholar
5.
Tien, J.K., Thompson, A.W., Bernstein, I.M., and Richards, R.J., Metall. Trans. A, 7A, 821(1976).Google Scholar
6.
Fidelle, J.P., Broudeur, R., Pellissier-Tanon, A., and Roux, C., Symposium, “Corrosion pous tension et fragilisation par 1' hydrogene, Paris, France, April, 23(1971).Google Scholar
7.
Dickson, J.I., Groulx, D.and Li, S.Q., Materials Science and Engineering, 94, 155(1987).Google Scholar
8.
Magnin, T., Lepinoux, J., in “Parkins Symposium on Fundamental Aspects of Stress Corrosion Cracking”, edited by Bruemmer, S.M., Meletis, E.I., Jones, R.H., Gerberich, W.W., Ford, F.P., and Staehle, R.W., The Minerals, Metals & Materials Society.
323(1992).Google Scholar
9.
Mukai, Y., Watanabe, M. and Murata, M., in Fractography in Failure analysis, ASTM STP 645, 164(1978)-Google Scholar
10.
Liu, R., Narita, N., Altstetter, C., Birnbaum, H. and Pugh, E.N., Metall. Trans. A,
11, 1563(1980).Google Scholar
12.
Chen, Q Z., Chu, W.Y., Qiao, L.J., Xiao, C.M., Chinese Science Bulletin,
39, 1329(1996).Google Scholar