Hostname: page-component-78c5997874-xbtfd Total loading time: 0 Render date: 2024-11-20T01:15:44.250Z Has data issue: false hasContentIssue false

Hot-die Forging of a β-stabilized γ-TiAl Based Alloy

Published online by Cambridge University Press:  28 August 2018

Wilfried Wallgram
Affiliation:
Bohler Schmiedetechnik GmbH & CoKG, Kapfenberg, Austria
Helmut Clemens
Affiliation:
Department of Physical Metallurgy and Materials Testing, Montanuniversität Leoben, Leoben, Austria
Sascha Kremmer
Affiliation:
Bohler Schmiedetechnik GmbH & CoKG, Kapfenberg, Austria
Andreas Otto
Affiliation:
GfE Metalle und Materialien GmbH, Nuremberg, Germany
Volker Güther
Affiliation:
GfE Metalle und Materialien GmbH, Nuremberg, Germany
Get access

Abstract

Because of the small “deformation window” hot-working of γ-TiAl alloys is a complex and difficult task and, therefore, isothermal forming processes are favoured. In order to increase the deformation window a novel Nb and Mo containing γ-TiAl based alloy (TNM alloy) was developed. Due to a high volume fraction of β-phase at elevated temperatures the alloy can be hot-die forged under near conventional conditions, which means that conventional forging equipment with minor and inexpensive modifications can be used. With subsequent heattreatments balanced mechanical properties can be achieved. This paper summarizes our progress in establishing a “near conventional” forging route for the fabrication of γ-TiAl components. The results of lab scale compression tests and forging trials on an industrial scale are included. In addition, the mechanical properties of forged and heat-treated TNM material are presented.

Type
Articles
Copyright
Copyright © Materials Research Society 2009

Access options

Get access to the full version of this content by using one of the access options below. (Log in options will check for institutional or personal access. Content may require purchase if you do not have access.)

References

1. Weimer, M. J., Kelly, T. J., Paper presented at the 3rd international Workshop on ©-TiAl Technologies, Bamberg, Germany, (March 28 – 31, 2006).Google Scholar
2. Appel, F., Paul, J. D. H., Oehring, M., Buque, C., in: Gamma Titanium Aluminides 2003, eds. Kim, Y.-W., Clemens, H., Rosenberger, A. H. (The Minerals, Metals and Materials Society (TMS), Warrendale, 2003), pp. 139151.Google Scholar
3. Kremmer, S., Chladil, H. F., Clemens, H., Otto, A., and Güther, V., in Ti-2007 Science and Technology, Vol. 2, The Japan Institute of Technology, Japan 2008, 989.Google Scholar
4. Güther, V., Otto, A., Klose, J., Rothe, C., Clemens, H., Kachler, W., Winter, S., Kremmer, S., in: Structural Aluminides for Elevated Temperature Applications, eds. Kim, Y.-W., Morris, D., Yang, R., Leyens, C., (The Minerals, Metals and Materials Society (TMS), Warrendale, 2008), pp. 249-256.Google Scholar
5. Clemens, H., Boeck, B., Wallgram, W., Schmoelzer, T., Droessler, L. M., Zickler, G. A., Leitner, H., Otto, A., these proceedings.Google Scholar
6. Appel, F., Kestler, H. and Clemens, H., in: Intermetallic Compounds – Principles and Practice, Volume 3, Progress, eds.: Westbrook, J. H. and Fleischer, R. L. (Chicester, UK: John Wiley Publishers, 2002), 617642.Google Scholar
7. Clemens, H., Wallgram, W., Kremmer, S., Güther, V., Otto, A., Bartels, A., Adv. Eng. Mater. 10, 707 (2008).Google Scholar
8. Chladil, H. F., Ph.D. thesis, Montanuniversität, Leoben, Austria 2007.Google Scholar
9. Clemens, H., Chladil, H.F., Wallgram, W., Zickler, G.A., Gerling, R., Liss, K.-D., Kremmer, S., Güther, V., Smarsly, W., Intermetallics 16, 827 (2008).Google Scholar
10. Droessler, L.M., Schmoelzer, T., Wallgram, W., Cha, L., Das, G., Clemens, H., these proceedings.Google Scholar