Hostname: page-component-78c5997874-xbtfd Total loading time: 0 Render date: 2024-11-04T21:27:10.815Z Has data issue: false hasContentIssue false

Highly Stable Ir-Ta-O Electrode for Ferroelectric Material Deposition

Published online by Cambridge University Press:  21 March 2011

Fengyan Zhang
Affiliation:
Sharp Laboratories of America, Inc., 5700 NW Pacific Rim Blvd. Camas, WA 98607, USA
Sheng Teng Hsu
Affiliation:
Sharp Laboratories of America, Inc., 5700 NW Pacific Rim Blvd. Camas, WA 98607, USA
Jer-shen Maa
Affiliation:
Sharp Laboratories of America, Inc., 5700 NW Pacific Rim Blvd. Camas, WA 98607, USA
Yoshi Ono
Affiliation:
Sharp Laboratories of America, Inc., 5700 NW Pacific Rim Blvd. Camas, WA 98607, USA
Ying Hong
Affiliation:
Sharp Laboratories of America, Inc., 5700 NW Pacific Rim Blvd. Camas, WA 98607, USA
Weiwei Zhuang
Affiliation:
Sharp Laboratories of America, Inc., 5700 NW Pacific Rim Blvd. Camas, WA 98607, USA
Shigeo Ohnishi
Affiliation:
Sharp Corporation, Tenri-city, Nara632-8567, Japan
Wendong Zhen
Affiliation:
Sharp Corporation, Tenri-city, Nara632-8567, Japan
Norito Fujiwara
Affiliation:
Sharp Corporation, Tenri-city, Nara632-8567, Japan
Get access

Abstract

Ir-Ta-O composite bottom electrode has extraordinary high temperature stability. It can maintain good conductivity and integrity even after 5min annealing at 1000 °C in oxygen ambient. The thermal stability of Ir-Ta-O on different substrates has been studied. It shows that Ir-Ta-O is also very stable on Si and SiO2 substrates. No hillock formation and peelings of the bottom electrode were observed after high temperature and long time annealing in O2 ambient. SEM, TEM, XRD, and AES have been used to characterize the Ir-Ta-O film and the interfaces between Ir-Ta-O bottom electrode and Si or SiO2 substrate. The composition and conductivity changes of the electrode during oxygen ambient annealing and the interdiffusion issue will be discussed. Furthermore, Ir-Ta-O/SiO2/Si capacitor with 30Å gate oxide was fabricated and the C-V and I-V characteristics were measured to confirm the stability of Ir-Ta-O on thin gate oxide.

Type
Research Article
Copyright
Copyright © Materials Research Society 2001

Access options

Get access to the full version of this content by using one of the access options below. (Log in options will check for institutional or personal access. Content may require purchase if you do not have access.)

References

1) Hren, P.D., Rou, S. H., Al-Shareef, H. N., Gifford, K.D., Auciello, O., and Kinggon, A.I., Integarated Ferroelectrics, 2, 311 (1992)Google Scholar
2) Olowolafe, J.O., Jones, R. E., Campbell, A.C., Maniar, P.D., Hegde, R.I., and Mogab, C.J., Mat Res Soc. Symp. Proc., 243, 355 (1992)Google Scholar
3) Nakamura, T., Nakao, Y., Kamisawa, A. and Takasu, H., Appl. Phys. Lett. 65, 1522 (1994)Google Scholar
4) Nakamura, T., Nakao, Y., Kamisawa, A. and Takasu, H., Jpn. J. Appl. Phys. Lett. 33, 5207 (1994)Google Scholar
5) Zhang, Fengyan, Li, Tingkai, Nguyen, Tue, Hsu, Sheng Teng, Ferroelectric Thin Films VII, Mat Res Soc. Symp. Proc (1998) (to be published)Google Scholar
6) Kim, Seung-Hyun, Hong, J.G., Gunter, J.C., Lee, H. Y., Streiffer, S.K, and Kingon, Angus I., Mat Res Soc. Symp. Proc. 493, 131(1997)Google Scholar
7) Bai, G. -R., Wang, A., Tsu, I-Fei, Foster, C.M., and Auciello, O., Integarated Ferroelectrics, 21, 291 (1998)Google Scholar
8) Grill, A., Laibowitz, R., Beach, D., Neumayer, D. and Duncombe, P.R., Integarated Ferroelectrics, 14, 211 (1997)Google Scholar
9) Aoki, Katsuhiro, Fukuda, Yukio, Numata, Ken, and Nishimura, Akitoshi, Jpn. J. Appl. Phys. Vol. 34, 5250 (1995)Google Scholar
10) Lee, J.J., Thio, C. L., and Desu, S.B., J. Appl. Phys. 78(8) 5073 (1995)Google Scholar
11) Wolf, S., Silicon Processing, Lattice Press (Sunset Beach, California, 1990), Vol. 2, p271 Google Scholar
12) Yoon, Dong-Soo, Baik, Hong Koo, Lee, Sung-Man, Lee, Sang-In, Hwack, Hyun and Lee, Joo, J. Vac. Sci. Technol. B 16(3), May/Jun, 1137(1998)Google Scholar
13) Yoon, Dong-Soo, Baik, Hong Koo, Lee, Sung-Man, Lee, Sang-In, , Hyun and Lee, Hwack Joo, Appl. Phys. Lett. V 73, 324 (1998)Google Scholar
14) Horng, Ray-Hua, Wuu, Dong-Sing, Wu, Luh-Huei, Lee, Ming-Kwei, Chan, Shih-Hsiung, LEU, Ching-Chich, Huang, Tiao-Yuan and SZE, Simon Min, Jpn. J. Appl. Phys., 37, L1274 (1998)Google Scholar
15) Wickenden, D.K., Sisson, M. J., Todd, A. G., and Kelly, M.J., Solid State Electronics, 27, 515 (1984)Google Scholar
16) Zhang, Fengyan, Maa, Jershen, Hsu, Sheng Teng, Ohnishi, Shigeo and Zhen, Wendong, Jpn. J. Appl. Phys. 38, L1447 (1999)Google Scholar