Hostname: page-component-586b7cd67f-dlnhk Total loading time: 0 Render date: 2024-11-22T07:00:17.845Z Has data issue: false hasContentIssue false

Effects of Si and Ni nanoparticles in Brazing process on fracture surfaces of 304 stainless steels

Published online by Cambridge University Press:  28 February 2012

H. M. Hdz-García
Affiliation:
Corporación Mexicana de Investigación en Materiales, Calle Ciencia y Tecnología No. 790 Fracc. Saltillo 400; Saltillo, Coah. CP. 25290. e-mail: [email protected].
J. L. Acevedo-Dávila
Affiliation:
Corporación Mexicana de Investigación en Materiales, Calle Ciencia y Tecnología No. 790 Fracc. Saltillo 400; Saltillo, Coah. CP. 25290. e-mail: [email protected].
L. A. García-Cerda
Affiliation:
Centro de Investigación de Química Aplicada, Blvd. Enrique Reyna Hermosillo, Saltillo, Coah.
M. I. Pech-Canul
Affiliation:
Centro de Investigación y Estudios Avanzados del IPN, Carr. Monty-Saltillo km. 13; Ramos Arizpe, Coah. CP. 25900.
R. Muñoz-Arroyo
Affiliation:
Centro de Investigación y Estudios Avanzados del IPN, Carr. Monty-Saltillo km. 13; Ramos Arizpe, Coah. CP. 25900.
F. A. Reyes-Valdes
Affiliation:
Corporación Mexicana de Investigación en Materiales, Calle Ciencia y Tecnología No. 790 Fracc. Saltillo 400; Saltillo, Coah. CP. 25290. e-mail: [email protected].
F. A. Hernández-García
Affiliation:
Universidad Politécnica de Querétaro carr. Est. 420 s/n; El Marques, Qro. C.P. 76240.
J. A. Aguilar-Martínez
Affiliation:
Centro de Investigación en Materiales Avanzados, Alianza Norte 202, Autopista Mty-Aeropuerto Km. 10, Parque de Investigación e Innovación Tecnológica (PIIT), Apodaca, NL, C.P. 66600
Get access

Abstract

In order to increase the wettability and capillary forces of the filler metal between micro-cracking and micro-porous on the fracture surfaces of 304 stainless steels, methods of impregnation of Si and growth of Ni nanoparticles were used. These nanoparticles have a role inside the Transient Liquid Phase (TLP) and the substrate when using Brazing process. TLP can react with the nanoparticles previously deposited between micro-cracking and micro-porous and therefore promotes the nucleation and growth sites of phases and decreases the formation of eutectic structures. This method increases the effectiveness of metallic components reparation using Brazing process. Such effectiveness is indicated by an inspection of microstructural failure analysis, as a first stage, in the covered zone by the filler metal.

Type
Articles
Copyright
Copyright © Materials Research Society 2012

Access options

Get access to the full version of this content by using one of the access options below. (Log in options will check for institutional or personal access. Content may require purchase if you do not have access.)

References

[1] Lippold, J.C, Kotecki, D.J,. Austenitic Stainless Steels, edited by Lippold, JC., Kotecki, DJ, (Wiley-Interscience, New Jersey, 2005); p. 142144.Google Scholar
[2] Xiaowei, Wu, Chandel, R.S, Hang, Li, J. Mater. Sc. 36, 153156 (2001).Google Scholar
[3] Nakahashi, M. J., Jpn. Inst. Met., 49 (No. 4), 285290 (1985).Google Scholar
[4] Sjodin, P., Wolfe, C., Wilhelmesson, B., “A noval type of all-stainless steel plate heat exchangers”, (Proc. Of 5 Int. Conf. on Enhanced, Comp., and Ultra-Comp. Heat Exch.: Sci. Eng. and Tech, New Jersey, ed. Shah, R.K., 2005), 215–220.Google Scholar
[5] Jang, J.S, Shih, H.P.,. J. of Mater. Sc. Lett. 22, 7982 (2003).Google Scholar
[6] Arafin, M. A., Medraj, M., Turner, D. P., Bocher, P., Mater. Sc. and Engineering A447, 125133, (2007).Google Scholar
[7] Cook, G. O. III, Sorensen, C. D., J. Mater Sci. 46, 53055323 (2011).Google Scholar
[8] Stephen, L., Proc. of the 3rd Int. Brazing and Soldering Conference, (April 24-26, San Antonio, Texas 2006) pp. 334337.Google Scholar
[9] Poffo, M. C., de Lima, C. J., Souza, S. M., Triches, D. M., Grandi, T. A.., de Biasi, R., J. Raman Spec. 22 Dec, 1606-1609 (2009).Google Scholar
[10] Nebol´sin, V. A., Schetinin, A. A., Korneeva, A. N., Dunaev, A. I., Dolgachev, A. A., Sushko, T. I., Tatarenkov, A. F., Inor. Mater. 4, 339345 (2006).Google Scholar
[11] Geng, G., Lin, , Li-na, L., Kui-ming, . Trans. Nonferrous Met. Soc. China 20, 349354 (2010).Google Scholar
[12] Shibutani, T., IEEE Trans., 3, 177182 (2010).Google Scholar
[13] Arafin, M. A., Medraj, M., Turner, D. P., Bocher, P., Mater. Chem. and Phys. 106, 109119 (2007).Google Scholar