Effect of Simulated Body Fluid on the Microstructure of Ferrimagnetic Bioglass-Ceramics
Published online by Cambridge University Press: 01 February 2011
Abstract
The effect of simulated body fluid (SBF) on the structure and microstructure of ferrimagnetic bioglass ceramics (FBC) was investigated in series of samples in the system of the oxides [0.45(CaO, P2O5) (0.52-x)SiO2 xFe2O3 0.03Na2O], with X = 0.05, 0.10, 0.15, 0.20. Physical properties of the materials were studied as a function of processing parameters and time of immersion in SBF by x-ray diffraction (XRD) and scanning electron microscopy (SEM) with energy dispersive x-ray spectroscopy (EDS). The in vitro experiment showed that bioactivity of the FBC varies with the composition of the oxides, heat treatment, and time of exposure in SBF in a non-systematic way. A surface layer of Si, P, Ca partially covers the Fe, O dendrites, while formation and size of pores is determined by the specific processing parameters of the materials.
- Type
- Research Article
- Information
- Copyright
- Copyright © Materials Research Society 2004