Effect of Bn Interfacial Coating on the Strength of a Silicon Carbide/Silicon Nitride Composite

Published online by Cambridge University Press:  15 February 2011

Kirk P. Norton
Affiliation:
General Atomics, P.O. Box 85608, San Diego, CA 92186–9784
Holger H. Streckert
Affiliation:
General Atomics, P.O. Box 85608, San Diego, CA 92186–9784
Get access

Abstract

Boron nitride has been identified as a good fiber/matrix interface coating for SiC fibers in a Si3N4 matrix. Boron nitride thin films prepared from BCl3 and NH3 at 1000°C and from B2 H6 and NH3 at 550°C were deposited on SiC (Nicalon®) cloth in a low pressure chemical vapor deposition reactor. The coating thickness was varied from 0.1 μm up to 4 μm. Six layers of cloth for each coating thickness were incorporated into a chemical vapor infiltrated matrix of amorphous Si3N4.

Flexural strength data and composite toughness were obtained from three-point bend tests. Scanning electron microscopy and metallographic analysis of fracture surface morphology were used to determine the failure mode.

Type
Research Article
Copyright
Copyright © Materials Research Society 1992

Access options

Get access to the full version of this content by using one of the access options below. (Log in options will check for institutional or personal access. Content may require purchase if you do not have access.)

References

1. Prewo, K. M.,“FIBER-REINFORCED CERAMICS: NEW OPPORTUNITIES FOR COMPOSITE MATERIALS,” 68 [2] 395400 (1989)Google Scholar
2. Kerans, R. J., Hay, R. S., Pagano, N. J., and Parthasarathy, T. A.,“THE ROLE OF THE FIBER-MATRIX INTERFACE IN CERAMIC COMPOSITES,” Ceramic Bulletin, 68 [2] 429–42 (1989)Google Scholar
3. Singh, R. N. and Brun, M. K.,“EFFECT OF BORON NITRIDE COATING ON FIBER-MATRIX INTERACTIONS,” Advanced Ceramic Materials, 3 [3] 235–37 (1988)Google Scholar
4. Lewis, D. III,” STRENGTH AND TOUGHNESS OF FIBER-REINFORCED CERAMICS AND RELATED INTERFACE BEHAVIOR,” Proceedings of ” Whisker-and Fiber-Toughened Ceramics,” Ed. by Bradley, R. A., etal., Oak Ridge, Tenn., 265273 (June 1988)Google Scholar
5. Brun, M. K. and Singh, R. N.,“EFFECT OF THERMAL EXPANSION MISMATCH AND FIBER COATING ON THE FIBER/MATRIX INTERFACIAL SHEAR STRESS IN CERAMIC MATRIX COMPOSITES,” Advanced Ceramic Materials, 3 [5] 506509 (1988)CrossRefGoogle Scholar
6. Lowden, R. A. and More, K. L.,“THE EFFECT OF FIBER COATINGS ON INTERFACIAL SHEAR STRENGTH AND THE MECHANICAL BEHAVIOR OF CERAMIC COMPOSITES,” MRS Symposium Proceedings, Vol.170 (1990)Google Scholar
7. Gulden, T. D., Hazlebeck, D. A., Norton, K. P., and Streckert, H. H.,“CERAMIC FIBER COATING BY GAS-PHASE AND LIQUID-PHASE PROCESSES,” Ceram. Eng. Sci. Proc. 11 [9–10] 1539–53 (1990)Google Scholar