Hostname: page-component-586b7cd67f-2brh9 Total loading time: 0 Render date: 2024-11-29T09:16:20.485Z Has data issue: false hasContentIssue false

Defects in 4H-SiC Induced by High Energy Helium Implantation

Published online by Cambridge University Press:  21 March 2011

Marie F. Beaufort
Affiliation:
Laboratoire de Métallurgie Physique UMR6630, BP30179, 86960Chasseneuil-Futuroscope, France
Erwan Oliviero
Affiliation:
Laboratoire de Métallurgie Physique UMR6630, BP30179, 86960Chasseneuil-Futuroscope, France
Marie L. David
Affiliation:
Laboratoire de Métallurgie Physique UMR6630, BP30179, 86960Chasseneuil-Futuroscope, France
Alain Declémy
Affiliation:
Laboratoire de Métallurgie Physique UMR6630, BP30179, 86960Chasseneuil-Futuroscope, France
Christian Blanchard
Affiliation:
Laboratoire de Métallurgie Physique UMR6630, BP30179, 86960Chasseneuil-Futuroscope, France
Esidor Ntsoenzok
Affiliation:
CNRS-CERI, 4A rue de la Férollerie, Orléans
Jean F. Barbot
Affiliation:
Laboratoire de Métallurgie Physique UMR6630, BP30179, 86960Chasseneuil-Futuroscope, France
Get access

Abstract

1.6 MeV He+ ions were implanted at room temperature into (0001) 4H-SiC at a dose of 1×1017 cm−2 and then annealed at 1500°C for 30 min. Small bubbles are readily observed in the as-implanted sample but also an amorphous layer. After a 1500°C annealing, recrystallization of the amorphous state occurs and large bubbles or cavities are observed. However their shape strongly depends of their location inside the buried layer. The recrystallization consists of polytypisme, 4H-SiC growth along the c-direction from the substrate, columnar 4H-SiC and epitaxial growth of 3C-SiC.

Type
Research Article
Copyright
Copyright © Materials Research Society 2001

Access options

Get access to the full version of this content by using one of the access options below. (Log in options will check for institutional or personal access. Content may require purchase if you do not have access.)

References

REFERENCES

1. Follstaedt, D.M., Myers, S.M., Petersen, C.A. and Medernach, J.W., J. Elect. Mat., 25, 157 (1996)Google Scholar
2. Raineri, V., Fallica, G. and Libertino, S., J. Appl. Phys., 79, 9012 (1996)Google Scholar
3. Spitnagel, J.A., Wood, S., Choyke, W.J., Doyle, N.J., Bradshaw, J. and Fishman, G., Nuc. Inst. and Meth. B, 16, 237 (1996)Google Scholar
4. Ishimaru, M., Harada, S., Motooka, T., Nakata, T., Yoneda, T. and Inoue, M., Nucl. Inst. and Meth. B, 127/128, 195 (1997)Google Scholar
5. Heera, V., Stoemenos, J., Kögler, R. and Skorupa, W., J. Appl. Phys., 77, 2999 (1995)Google Scholar
6. Ziegler, J.F., Biersack, J.P. and Littmark, U., the stopping and Range of Ions in Solids, Pergamon Press, New York (1985)Google Scholar
7. Chen, J., Chung, P. and Trinkaus, H., Phys. Rev. B, 61, 12923 (2000)Google Scholar
8. Harada, S., Ishimaru, M., Motooka, T., Nakata, T., Yoneda, T. and Inoue, M., Appl. Phys. Lett., 69, 23 (1996)Google Scholar