Published online by Cambridge University Press: 15 February 2011
Possibility of highly waste loaded borosilicate glasses up to 65wt% were investigated for HLW. In the case the waste was loaded at a content higher than 45wt%, apatite crystal was identified in the glasses. Adding above 2.5wt% of M0O3, yellow phase was observed in the 45wt% waste glass. In the case the composition of actual waste was simulated, waste(25–45wt%) glasses were characterized. Chemical durability of 45wt% waste glass was equivalent to that of 25wt% waste glass under the condition of Na20 content lower than 12wt%. Rheological behavior of 45wt% waste glass was equivalent to that of 25wt% waste glass in the range of melting temperature. Electrical resistivity of 45wt% waste glass were a little lower than that of 25wt% waste glass and it depended on the noble metal content. The Time-Temperature-Transformation (T-T-T) diagram and the leach rate of heat treated glass indicated a good thermal stability of highly waste loaded glass below the glass transition temperature. Possibility of high waste loading up to 45wt% was elucidated.