Article contents
Anomalous Diffusion of Intrinsic Defects in K+ Implanted ZnO using Li as Tracer
Published online by Cambridge University Press: 20 March 2012
Abstract
Potassium (K) ions have been implanted in hydrothermally grown ZnO to a dose of 1 × 1015 cm-2, followed by isochronal annealing in a tube furnace (30min) and by rapid thermal annealing (30s) on two separate samples. For annealing temperatures below 700°C, only a minor redistribution of Li is observed behind the projected range of the K+ ions. At temperatures between 700 and 750°C, however, both annealing treatments show a wide region behind the implantation peak which is depleted of Li, and this depletion is used as a tracer to monitor diffusion of intrinsic defects like the Zn interstitial. The results are interpreted as Zn interstitials being released from the implanted region in a burst at temperatures above ∼700°C, followed by rapid migration, replacement of Li on Zn site through the kick-out mechanism, and migration of Li away from the active region.
Keywords
- Type
- Research Article
- Information
- MRS Online Proceedings Library (OPL) , Volume 1394: Symposium M – Oxide Semiconductors–Defects, Growth and Device Fabrication , 2012 , mrsf11-1394-m01-02
- Copyright
- Copyright © Materials Research Society 2012
References
REFERENCES
- 2
- Cited by