Analogues for the Corrosion-induced Expansion of Iron in HLW containers

Published online by Cambridge University Press:  01 February 2011

Nicholas R. Smart
Affiliation:
Serco Assurance, Culham Science Centre, Abingdon, Oxfordshire, OX14 3ED, U.K.
Rachel Adams
Affiliation:
Serco Assurance, Culham Science Centre, Abingdon, Oxfordshire, OX14 3ED, U.K.
Lars Werme
Affiliation:
SKB, Box 5864, SE-10240, Stockholm, Sweden.
Get access

Abstract

In Sweden, spent nuclear fuel will be encapsulated in sealed cylindrical canisters, consisting of a cast iron insert and a copper outer container. The canisters will be placed in a deep geologic repository and surrounded by bentonite. If a breach of the outer copper container were to occur the cast iron insert would undergo anaerobic corrosion, forming a magnetite film whose volume would be greater than that of the base metal. In principle there is a possibility that accumulation of iron corrosion product could cause expansion of the copper canister. Anaerobic corrosion rates are very slow, so in the work described in this paper reference was made to analogous archaeological materials that had been corroding for long periods in natural anoxic aqueous environments. This paper describes a number of archaeological artefacts containing iron and copper corroding in constrained geometries in anoxic natural waters. No evidence has been obtained which would suggest that severe damage is likely to occur to waste canisters as a result of expansive corrosion of cast iron under repository conditions.

Type
Research Article
Copyright
Copyright © Materials Research Society 2004

Access options

Get access to the full version of this content by using one of the access options below. (Log in options will check for institutional or personal access. Content may require purchase if you do not have access.)

References

REFERENCES

1. Smart, N.R., Bond, A.E., Crossley, J.A.A., Lovegrove, P.C. and Werme, L., In Scientific Basis for Nuclear Waste Management XXIV, edited by Hart, K.P. and Lumpkin, G.R., (Mat. Res. Soc. Symp. Proc. 663, Warrendale, PA, 2001) pp. 477485.Google Scholar
2. Smart, N.R., Rance, A.P., Fennell, P. and Werme, L., Expansion Due To Anaerobic Corrosion of Steel and Cast Iron: Experimental and Natural Analogue Studies, Presented at International Workshop on Prediction of Long Term Corrosion Behaviour in Nuclear Waste Systems, Cadarache, November 2001.Google Scholar
3. Smart, N.R., Blackwood, D.J. and Werme, L., Anaerobic Corrosion of Carbon Steel and Cast Iron in Artificial Groundwaters: Part 2-Gas Generation, Corrosion 58(8), 627, 2002.Google Scholar
4. Johnson, A.B. and Francis, B., Durability of Metals from Archaeological Objects, Metal Meteorites and Native Metals, Battelle Pacific Northwest Laboratory, PNL-3198, 1980.Google Scholar
5. Tweddle, D., The Anglian Helmet from Coppergate, in The Archaeology of York Volume 17: The Small Finds, edited by Addyman, P.V. and Kinsler, V.A., (Council for British Archaeology publishers, London, 1992).Google Scholar
6. S.A., O'Connor, Conservation of the Helmet and Mail, in The Archaeology of York Volume 17: The Small Finds, edited by Addyman, P.V. and Kinsler, V.A., (Council for British Archaeology publishers, London, 1992), pp. 907.Google Scholar
7. Rule, M., The Mary Rose, The Excavation and Raising of Henry VIII's Flagship, Conway Maritime Press, 2nd edition, 1983.Google Scholar